Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 250 °C | 482 °F | STN EN 11357-1 |
Plastcom SLOVASTER® B1 GF 15 FRL 4 PBT reinforced with glass fibers, flame retarded PBT reinforced with 15 % glass fiber, flame retarded with the halogen flame retardant. Anisotropy of shrinkage enables the injection molding of round, cylindrical or other hole products. Application.. |
|||
Melting Point | 250 - 258 °C | 482 - 496 °F | DSC @ 15°C / min; ASTM D3418 |
Ovation Polymers RIGITRON 30545 GF Polyester, 45% Glass Reinforced Polyester – 45% Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Var.. |
|||
Melting Point | 250 °C | 482 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman 9663 PET
(discontinued **) VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers.. |
|||
Melting Point | 250 °C | 482 °F | |
Polyram PlusTek PA517 Nylon 6.6, Flame Retardant Flame retardant halogen free polyamide 6.6 formulated to meet V-0, for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 250 - 256 °C | 482 - 493 °F | |
Tisan TISAPET® 20% Glass Reinforced Polyethylene Terephthalate Properties:Excellent mechanical propertiesHigh thermal-chemical friction resistanceGood electrical propertiesGood rate of melt flow index relative to the quantity of glass fiberBalanced electrical a.. |
|||
Melting Point | 250 - 256 °C | 482 - 493 °F | |
Tisan TISAPET® 30% Glass Reinforced Polyethylene Terephthalate Properties:Excellent mechanical propertiesHigh thermal-chemical friction resistanceGood electrical propertiesGood rate of melt flow index relative to the quantity of glass fiberBalanced electrical a.. |
|||
Melting Point | 250 °C | 482 °F | ISO 3146 |
Wellman Wellpet® GF100-N1 30% Glass Fiber Reinforced, Natural PET Description: Glass Fiber Reinforced, Natural PETInformation provided by Wellman. |
|||
Melting Point | 250 °C | 482 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: .. |
|||
Melting Point | 250 °C | 482 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |
|||
Melting Point | <= 250 °C | <= 482 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Melting Point | <= 250 °C | <= 482 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q150-D PA410 Low/Medium Viscosity |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-HG10 PA410-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-HG6 PA410-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-HGM24 PA410-(GF+MD)30 10% Glass Reinforced, 20% Mineral Reinforced, Heat Stabilized |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-HXGM24 PA410-(GF+MD)30 % Glass Reinforced, % Mineral Reinforced, Heat Stabilized |
|||
Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
DSM EcoPaXX® Q-X07290 PA410-I Impact Modified |
|||
Melting Point | 250 °C | 482 °F | [10 K/min], ISO 11357 |
Eurotec® Tecopet® PT74 CR20 BK111 PR PET, 20% carbon fiber reinforced, black, fast crystallization grade Information provided by Eurotec® |
|||
Melting Point | 250 °C | 482 °F | [10 K/min], ISO 11357 |
Eurotec® Tecopet® PT74 GR20 BK002 DA PET, 20% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Melting Point | 250 °C | 482 °F | [10 K/min], ISO 11357 |
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Melting Point | 250 °C | 482 °F | [10 K/min], ISO 11357 |
Eurotec® Tecopet® PT74 GR30 BK002 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Melting Point | 250 °C | 482 °F | 10 K/min |
BASF Petra® 330 FR BK-112 30% Glass Filled PET Petra 330 FR BK-112 is a 30% glass reinforced, flame retardant PET, pigmented black injection molding compound rated UL94 V-0 in a 1/64 inch thickness. The product is designed for injection molding.. |
|||
Melting Point | 250 °C | 482 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr.. |
|||
Melting Point | 250 °C | 482 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri.. |