ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, North America and South America Additive: Antiblock: 7000 ppmSlip: NoProcessing Aid: NoThermal Stabilizer: YesApplications: Agricultural FilmBag in BoxBarrier Food PackagingBlown FilmBread BagsFood packagingForm Fill and Seal PackagingFreezer FilmGarment FilmGeneral PackagingHeavy Duty BagsIce BagsIndustrial LinersIndustrial PackagingLamination FilmLinersMultilayer Packaging FilmPackaging FilmsProduce BagsRefuse BagsShoppersStand Up PouchesTrash BagsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ExxonMobil method
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 7000 ppm
7000 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
Film Elongation at Break, MD 580 %
580 %
ASTM D882
Film Elongation at Break, TD 850 %
850 %
ASTM D882
Puncture Energy 3.16 J
2.33 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 80 g
80 g
ASTM D1922
Elmendorf Tear Strength TD 400 g
400 g
ASTM D1922
Dart Drop Test 100 g
0.221 lb
ASTM D1709A
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
Film Tensile Strength at Break, TD 35.2 MPa
5100 psi
ASTM D882
1% Secant Modulus, MD 193 MPa
28000 psi
ASTM D882
1% Secant Modulus, TD 221 MPa
32000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 250 °C
<= 482 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003
Gloss 45 %
45 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 10 lbf
ExxonMobil Method