Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 8700X Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 87768 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 87771 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion L0111 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion L1101 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion L9630 Polyvinyl Chloride, Rigid (PVC, Rigid) Product can meet UL-94V-0. Material passed V-0 @ 1.5mm in screening test at PDI.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C6850REC PC+ABS (Europe-Africa-Middle East) PC+ABS Industrial quality. Flame retardant. Limited colors only (Black and Grey)This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ HTX 92052 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C | 37.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid) Interior application for thick & thin gauge profile application.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX DS0036I PC LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, No.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Faradex DS0036IP PC LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Asia Pacific) LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Isoplast® 2520 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 2520 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include excel.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML3021A PC (Europe-Africa-Middle East) LEXAN ML3021A is a high viscosity, UV stabilised grade especially designed for injection blow moulding and profile extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp WFL32 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL32 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
37.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DX98477 PC LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RX06027 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RX06027 is a compound based on PA 66 containing Glass Bead. Added features include: Easy Molding, Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-A.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
37.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP YF002 POLYESTER ELASTOMER LNP* THERMOCOMP* YF002 is a compound based on Poyester Elastomer containing 10% Glass Fiber. Added feature of this grade is: High Modulus. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® EL-700 Polycarbonate + Polyester Blend Key Features:Flame retarding agentUnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® UT-400 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® UT-403 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RX06027 PA66, 30% Glass Filled, Injection Molded Staramide RX06027 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S34/8)Information provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Tyril® 880B SAN TYRIL® 880B SAN copolymer combines the high levels of chemical resistance, heat resistance and overall strength of 880 resin with improved mold flow and mold release characteristics.Data provided b.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makroblend® UT-250 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Tyril® 1000B SAN TYRIL® 1000B SAN copolymer offers the best balance of physical properties of all TYRIL grades. It also provides excellent processability and chemical resistance, superior heat resistance, and good .. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Tyril® 1011 SAN TYRIL® 1011 SAN copolymer is a light stabilized general purpose injection molding resin available in crystone color only. It exhibits excellent weathering characteristics, high strength, good chemi.. |
|||
CTE, linear, Parallel to Flow | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Tyril® 880 SAN TYRIL® 880 SAN copolymer offers excellent physical properties incorporating the highest levels of chemical resistance, heat resistance and overall strength of any TYRIL grade.Data provided by Dow C.. |