Eurostar Staramide RX06027 PA66, 30% Glass Filled, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Eurostar Engineering Plastics
Trade Name Staramide
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Staramide RX06027 PA66, 30% Glass Filled, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Staramide RX06027 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S34/8)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
5 mm/min; ISO 527
Elongation at Yield 2.5 %
2.5 %
5 mm/min; ISO 527
Tensile Modulus 3.40 GPa
493 ksi
1 mm/min; ISO 527
Flexural Yield Strength 83.0 MPa
12000 psi
2 mm/min; ISO 178
Flexural Modulus 2.90 GPa
421 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80x10x4; ISO 179/1eA
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 67.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
37.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
37.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Processing Properties Metric English Comments
Zone 1 265 - 275 °C
509 - 527 °F
Zone 2 270 - 280 °C
518 - 536 °F
Zone 3 270 - 280 °C
518 - 536 °F
Melt Temperature 270 - 280 °C
518 - 536 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.15 %
0.15 %