Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 60.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 60.0 °C
140 °F
Rate B; ISO 306/B50
Premix Thermoplastics PRE-ELEC® PE 1294
PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
Vicat Softening Point 60.0 °C
140 °F
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber  (discontinued **)
A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 9.0 MPa (1300 psi); Vica..
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525
DuPont Bynel® 3062 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Vicat Softening Point 60.0 °C
140 °F
VST/B/50; ISO 306
MBA Polymers PP 2126 Post-consumer recycled general purpose polypropylene impact copolymer
Available in standard black.Information provided by MBA Polymers.
Vicat Softening Point 60.0 °C
140 °F
ISO 306
Lucobit Lucofin® 1400MN Powder Ethylene Butyl Acrylate
Lucofin 1400MN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN Powder is softer and more flexible ethane et..
Vicat Softening Point 60.0 °C

@Load 5.00 kg
140 °F

@Load 11.0 lb
LATI Latigea B01 F1 Bio-Polymer
Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr..
Vicat Softening Point 60.0 °C

@Load 5.00 kg
140 °F

@Load 11.0 lb
LATI Latigray 37 B01-01 CX/35 Bio-Polymer
Radiopaque compound based on Bio-Polymer (PLA, PHB, ...). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Vicat Softening Point 60.0 °C

@Load 5.00 kg
140 °F

@Load 11.0 lb
LATI Latilub 37 B01-02S Bio-Polymer
Self-lubricating product based on Bio-Polymer (PLA, PHB, ...). Silicone.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Vicat Softening Point 60.0 °C
140 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer
Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Vicat Softening Point 60.0 °C
140 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va..
Vicat Softening Point 60.0 °C
140 °F
50N-50°C per hour; ISO 306
Total PPC 9712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 9712 is heterophasic copolymer. PPC 9712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early de..
Vicat Softening Point 60.0 °C
140 °F
A50; DIN 53460
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525
DuPont Bynel® 2002 Acid-Modified Ethylene Terpolymer Adhesive Resin
Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature ..
Vicat Softening Point 60.0 °C
140 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer
Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing pro..
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer
Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films..
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525, ISO 306
DuPont™ Appeel® 20D875 Ethylene Acrylate
Appeel® 20D875 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad tempe..
Vicat Softening Point 60.0 °C
140 °F
B50 (50N); ISO 306
Domo 2500H Polypropylene Copolymer
Information provided by Domo.
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525
Dow Engage® 8003 Polyolefin Elastomer
Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer ..
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525, ISO 306
DuPont™ Appeel® 20D784 Ethylene Acrylate
Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature ..
Vicat Softening Point 60.0 °C
140 °F
50 N - B method; ISO 306
Arkema Group Orgalloy® LE 60LMXV Polyamide 6 Alloy
Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Vicat Softening Point 60.0 °C
140 °F
50°C/hr; 50N
Arkema Group Pebax® 2533 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 25 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525
C.O.I.M. LARIPUR® LPR7025 Special Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Vicat Softening Point 60.0 °C
140 °F
BASF Novolen® 3340 PC Polypropylene
Nucleated grade for injection moldings with higher transparency.Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 60.0 °C
140 °F
BASF Procom® GC20S 400 Polypropylene
Uses: electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 60.0 °C
140 °F
50°C/hr; 50N
Arkema Group Appryl® 3130 MU 7 Polypropylene - Polyethylene Copolymer
PP/PE copolymer colored during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive industry. It ..
Vicat Softening Point 60.0 °C
140 °F
B
Plastcom SLOVALEN PQ 83 T 40 PP, 40% mineral filling
FeaturesModified PP for injection moulding with the content of 40% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased ..
Vicat Softening Point 60.0 °C

@Load 5.00 kg
140 °F

@Load 11.0 lb
LATI Latimass 37 B01-01 D025 Bio-Polymer
Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Vicat Softening Point 60.0 - 156 °C
140 - 313 °F
Average value: 133 °C Grade Count:58
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
Vicat Softening Point 60.0 °C
140 °F
Mitsui NOTIO™ PN-2070 Nano-crystal Structure Controlled Elastomer
NOTIO™ is a polyolefin elastomer designed by a really new concept. NOTIO™ is a controlled crystal and amorphous structure on a nano scale, and shows better properties when compared with conventio..