Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 255 °C | 491 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66 Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app.. |
|||
Vicat Softening Point | 255 °C | 491 °F | 9.8 N; ASTM D1525 |
Nilit Polynil® P40 Low Viscosity Nylon 66 Description: Low viscosityApplication: CompoundingInformation provided by NILIT. |
|||
Vicat Softening Point | 255 °C | 491 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66 Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Vicat Softening Point | 255 °C | 491 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66 Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper.. |
|||
Vicat Softening Point | 255 °C | 491 °F | 50N; ISO 306 |
Grupo Repol Dinalon® A1S25 G30 PA66 30% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latistat 66-06 G/30 PA66, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Vicat Softening Point | 255 °C | 491 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
Vicat Softening Point | 255 °C | 491 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC006 is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 226F6 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has very high mechanical strength in combination with good flow properties. It shows hig.. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 226F7 Nylon 6.6, 35% Glass Fiber SAXAMID 226F7 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 35% glass fibers. It has very high mechanical strength in combination with good impact resistance. It is char.. |
|||
Vicat Softening Point | 255 °C | 491 °F | ISO 306 |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Vicat Softening Point | 255 °C | 491 °F | ISO 306 |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Vicat Softening Point | 255 °C | 491 °F | DAM; 50°C/h 50N; ISO 306 |
DuPont Performance Polymers Zytel® FG70G50HSLA BK309 Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Eurostar Staramide AG4 PA66, 20% Glass Filled, Injection Molded AG4 is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Eurostar Staramide AG5 PA66, 25% Glass Filled, Injection Molded AG5 is a 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Eurostar Staramide AG7H PA66, 35% Glass Filled, Injection Molded AG7 is a Heat Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 255 °C @Load 5.10 kg |
491 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 GR50 NL HS PA6.6, 50% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Eurostar Staramide RF006XXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006XXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006)Information provided by Eurostar. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 255 °C @Load 5.10 kg |
491 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NAX0 GR70 NL HS PA6.6, 70% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 255 °C | 491 °F | 50°C/h 50N; ISO 306 |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Vicat Softening Point | 255 °C | 491 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Vicat Softening Point | 255 °C | 491 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latilub 80-15T G/30 PPS, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latilub 80-17ST G/30 PPS, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |