| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced |
| Manufacturer | Nilit |
| Trade Name | Polynil® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Nilit Polynil® P40 Low Viscosity Nylon 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
| Water Absorption | 1.5 % | 1.5 % | 24h in H<sub>2</sub>O; sim. ISO 62 |
| Water Absorption at Saturation | 8.5 % | 8.5 % | sim. ISO 62 |
| Viscosity Measurement | 40 | 40 | relative viscosity (formic acid); ASTM D789 |
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | Nilit |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 80.0 MPa | 11600 psi | ASTM D638 |
| Tensile Modulus | 3.00 GPa | 435 ksi | ASTM D638 |
| Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
| Flexural Modulus | 2.85 GPa | 413 ksi | ASTM D790 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 225 °C | 437 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 85.0 °C | 185 °F | ASTM D648 |
| Vicat Softening Point | 240 °C | 464 °F | 49 N; ASTM D1525 |
| 255 °C | 491 °F | 9.8 N; ASTM D1525 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | >= 600 V | >= 600 V | UL 746 |