Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 225 °C @Load 5.10 kg |
437 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A ECP3808 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Vicat Softening Point | >= 225 °C | >= 437 °F | ASTM D1525 |
Covestro Petlon® 7530 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperat.. |
|||
Vicat Softening Point | >= 225 °C | >= 437 °F | ASTM D1525 |
Covestro Petlon® DP3-1018 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
Vicat Softening Point | >= 225 °C | >= 437 °F | ASTM D1525 |
Covestro Petlon® 4835 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
Vicat Softening Point | 225 - 255 °C | 437 - 491 °F | Average value: 240 °C Grade Count:4 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Vicat Softening Point | 225 - 255 °C | 437 - 491 °F | Average value: 241 °C Grade Count:25 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Vicat Softening Point | 225 °C | 437 °F | 50 N; 120 °C/h; ISO 306 |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Vicat Softening Point | 225 °C @Load 5.00 kg |
437 °F @Load 11.0 lb |
|
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Vicat Softening Point | 225 °C @Load 5.00 kg |
437 °F @Load 11.0 lb |
|
LATI Later 4 K/30 PBT, 30% Carbon Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti.. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2210 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2210R PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2210R PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2300F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact compliant. Effective June, 2007 this grade will no longer be supported with .. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2300R PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 2310 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 4000 PEI (Europe-Africa-Middle East) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS com.. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM HU2400 PEI 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM PW2300 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V9561 PET Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl GTX GTX8110P PPE+PA (Europe-Africa-Middle East) GTX8110P is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaksThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Asia Pacific) Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Vicat Softening Point | 225 °C | 437 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Vicat Softening Point | 225 °C | 437 °F | B/120; ISO 306 |
Eurostar Staramide AST42K PA66, Impact Modified, Injection Molded AST42K is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 225 °C | 437 °F | 10 N - A method; ISO 306 |
Arkema Group Orgalloy® RS 6600 Polyamide 6.6 Alloy Polyamide Alloy, Rigid grade, Nylon 6.6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |