Covestro Petlon® DP3-1018 Semi-Crystalline PET, 35% Mineral/Glass Fiber  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Petlon® DP3-1018 Semi-Crystalline PET, 35% Mineral/Glass Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 495-530°F, Mold Temperature: 195-250°F)Petlon® is manufactured by Albis Plastics Corporation and is a registered trademark of Bayer Corporation.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.
Physical Properties Metric English Comments
Density 1.74 g/cc
0.0629 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
(24 hr); ASTM D570
Moisture Absorption at Equilibrium 0.11 %
0.11 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 111.7 MPa
16200 psi
ASTM D638
Flexural Yield Strength 171 MPa
24800 psi
ASTM D790
Flexural Modulus 10.62 GPa
1540 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 140 °C
284 °F
RTI
Deflection Temperature at 1.8 MPa (264 psi) 228 °C
442 °F
ASTM D648
Vicat Softening Point >= 225 °C
>= 437 °F
ASTM D1525
UL RTI, Mechanical without Impact 140 °C
284 °F
Flammability, UL94 V-0
V-0
0.028 in
Electrical Properties Metric English Comments
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Arc Resistance 75 sec
75 sec
ASTM D495
Processing Properties Metric English Comments
Melt Temperature 257 - 277 °C
495 - 531 °F
Injection
Mold Temperature 91.0 - 121 °C
196 - 250 °F