Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 165 °C | 329 °F | ASTM D1525 |
Multibase Nylex™ 2185 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Vicat Softening Point | 165 °C | 329 °F | B |
Plastcom SLOVALEN PH 71 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 3413R PC (Asia Pacific) Lexan* resin 3413R is a flame retardant polycarbonate grade with 30% glass fiber reinforcement to meet UL 94 V1 listing at 1.5mm. This grade can be considered for applications requiring higher stiff.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 3414R PC (Asia Pacific) 40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Vicat Softening Point | 165 °C | 329 °F | ISO 306 |
Radici Radilon® SLVHPL128 (dry) Nylon 6 Plasticized for improved flexibilityInformation provided by Radici group. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 3412R PC (Asia Pacific) 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Vicat Softening Point | 165 - 220 °C | 329 - 428 °F | Average value: 208 °C Grade Count:18 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Vicat Softening Point | 165 °C | 329 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1850-7795 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Vicat Softening Point | 165 °C | 329 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80-8003 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latigray 82-03 CW/96 F3 PA 12, Metallic Reinforced Radiopaque compound based on Polyamide 12 (PA12). Metallic filler. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America;.. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latigray 82-04 CX/90 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latimass 82-02 D030 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latimass 82-03 D080 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latimass 82-06 D030 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East) Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea.. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Vicat Softening Point | 165 °C | 329 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East) NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50 N - B method; ISO 306 |
Arkema Group Orgalloy® RS 6600 Polyamide 6.6 Alloy Polyamide Alloy, Rigid grade, Nylon 6.6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Vicat Softening Point | 165 °C | 329 °F | under 1 daN; ASTM D1525 |
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo.. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AZM 23 G9 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,(G+C)(F+D)(23+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF23Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-rele.. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High.. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Vicat Softening Point | 165 °C | 329 °F | 50°C/hr; 50N |
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Conditioned) Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp.. |
|||
Vicat Softening Point | 165 °C | 329 °F | B |
Plastcom SLOVALEN PH 69 GF 40 PP, 40% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Vicat Softening Point | 165 °C @Load 5.00 kg |
329 °F @Load 11.0 lb |
|
LATI Latimass 82-05 D040 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |