| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced | 
| Manufacturer | Radici Group Plastics | 
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Radici Radilon® SLVHPL128 (dry) Nylon 6.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ISO 1183 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 40.0 MPa | 5800 psi | ISO 527-1/2 | 
| Elongation at Break | >= 50 % | >= 50 % | ISO 527-1/2 | 
| Elongation at Yield | 35 % | 35 % | ISO 524-1/2 | 
| Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1/2 | 
| Flexural Strength | 30.0 MPa | 4350 psi | ISO 178 | 
| Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 | 
| Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Melting Point | 217 °C | 423 °F | ISO 1135 7-1-3 | 
| Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ISO 75/2Bf | 
| Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75/2Af | 
| Vicat Softening Point | 165 °C | 329 °F | ISO 306 | 
| Flammability, UL94 | HB @Thickness 0.800 mm | HB @Thickness 0.0315 in |