Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
Plaskolite West Optix® CA-924 Impact Modified Acrylic Resin Injection Molding Grade Pellets. Good impact strength. |
|||
Vicat Softening Point | 112 °C | 234 °F | B |
Plastcom SLOVALEN PC 79 GF 20 PP, 20% glass fibre, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Vicat Softening Point | 112 °C @Load 1.00 kg |
234 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Flexirene® MR 50 A Linear Low Density Polyethylene Flexirene MR 50 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity... |
|||
Vicat Softening Point | 112 °C @Load 1.00 kg |
234 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Flexirene® MR 56 A Linear Low Density Polyethylene Flexirene MR 56 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity... |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East) CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb.. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® C2950HF PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced impact and heat properties plus improved flow for various applications. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Vicat Softening Point | 112 °C | 233 °F | ASTM D-1525 |
Plaskolite Optix® CP - 924 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 112 °C | 233 °F | ASTM D-1525 |
Plaskolite Optix® CP - 927 G High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate A, ASTM D1525 |
Plaskolite West Optix® CA-927 G Clear Impact Modified Acrylic Resin Impact modified acrylic resin, injection molding gradeApplications: An impact-modified acrylic resin designed for medical or food uses. This resin offers impact strengths up to seven times of gener.. |
|||
Vicat Softening Point | 112 °C | 233 °F | ASTM D-1525 |
Plaskolite West Optix® CP - 924 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
NOVA Chemicals Sclair® 8406 BK, 8406 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
NOVA Chemicals Sclair® 8406 UV8D, 8406G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Vicat Softening Point | 112 °C | 234 °F | 1 kg; ASTM D1525 |
LG Chemical HP PMMA Information Provided by LG Chem |
|||
Vicat Softening Point | 112 °C | 234 °F | ISO 306A |
Lucite International Diakon® Rapide CLG 910B Enhanced Molding Acrylic Polymer Specially designed to reduce injection molding cycle times and therefore provide production cost benefits.Information provided by Lucite International |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Vicat Softening Point | 112 °C | 234 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® NH-1037 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate "A" Loading 2 (50 degC/h 50N); ASTM Test |
Styrolution Terluran® HH-112 ABS Terluran HH-112 is an injection molding grade of ABS with very high heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr.. |
|||
Vicat Softening Point | 112 °C @Load 5.10 kg |
234 °F @Load 11.2 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTAPROP H0260 MC/EC Conductive Polypropylene, Mineral Filled Information provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 112 °C | 234 °F | ASTM D1525, ISO 306 |
DuPont™ Fusabond® P353 Polymer Modifier DuPont Fusabond® P353 is a chemically modified polypropylene. Uses: Automotive Applications Plastics Modification Polymer Modifier Applications: Coupling agent Long glass fiber filled PP compoun.. |
|||
Vicat Softening Point | 112 °C @Load 1.00 kg, Thickness 3.17 mm |
234 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers ABS 3500 EF-Low Gel Extrusion Grade, Low Gel Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 112 °C | 234 °F | |
Ineos ABS NOVODUR® P3TF ABS, Injection Grade
(discontinued **) Injection molding grade, improved flow.Applications: Automotive industry: e.g. wheel trims, instrument panel components.Information provided by the manufacturer.Novodur is produced by Styrolution (2.. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Asia Pacific) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Vicat Softening Point | 112 °C | 234 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Vicat Softening Point | 112 °C | 234 °F | ISO 306A |
Lucite International Diakon® ST15G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in.. |