Material Notes:
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D-955
Melt Flow 6.3 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.3 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength 58.4 MPa
8470 psi
ASTM D-638
Elongation at Break 4.6 %
4.6 %
ASTM D-638
Modulus of Elasticity 3.25 GPa
472 ksi
ASTM D-638
Flexural Strength 86.25 MPa
12510 psi
ASTM D-790
Izod Impact, Notched 0.320 J/cm

@Thickness 6.35 mm
0.600 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Gardner Impact 1.58 J

@Thickness 3.17 mm
1.17 ft-lb

@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C
38.9 µin/in-°F
ASTM D-696
Maximum Service Temperature, Air 50.0 °C
122 °F
UL-746 ABC
Deflection Temperature at 1.8 MPa (264 psi) 83.3 °C
182 °F
ASTM D-648
Vicat Softening Point 112 °C
233 °F
ASTM D-1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Haze <= 1.5 %
<= 1.5 %
ASTM D-1003
Transmission, Visible 91.6 %
91.6 %
ASTM D-1003