Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.90 GPa | 856 ksi | STN EN ISO 178 |
Plastcom SLOVAMID® 6 GF 20 FRA 5 PA6 reinforced with glass fiber, flame retarded PA 6 for injection molding, reinforced with 20% glass fiber, flame retarded with halogen flame retardant. Main features: flammability in accordance with UL 94 5 at 1.6 mm, glow wire at 960°C. Appli.. |
|||
Flexural Modulus | 5.90 GPa @Temperature 23.0 °C |
856 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYblend 85FS GF20 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
Shell Carilon® DB6F1G30 Polyketone, Flame-Retarded, Tracking-Resistant, Glass-Reinforced Injection Molding Grade
&n Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F1G30 is a flame-retarded, 15 percent glass-fiber-reinforced, injection molding grade with mecha.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
Nilit FRIANYL B63 FK 2010 Nylon 6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
NOVA Chemicals Dylark® 378P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 1.3 mm/min; ASTM D790 |
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant Vypet VNT 615 FR is a 15% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC STAMAX 30YM240 PP SABIC® STAMAX 30YM240 is a 30% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16496906... |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP SFL36 PA12 (Europe-Africa-Middle East) LNP* LUBRICOMP* SFL36 is a compound based on PA 12 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp PFB139E PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB139E is a compound based on PA 6 resin containing Glass Fiber, Glass Bead, Flame Retardant. Added features include; Flame Retardant, Easy Molding.This data was supplied by SABIC-.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 LNP* THERMOCOMP* RF0029S is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific) LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 226F4 Nylon 6.6, 20% Glass Fiber SAXAMID 226F4 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, Conditioned Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
Polyram RamOfin PPH308G6 Polypropylene, 30% Glass Fiber, Impact Modified 30% Glass fiber reinforced, heat stabilized, impact modified polypropylene for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam PFB139E PA6, Glass Fiber/Bead Filled, Flame Retardant, Injection Molded Starflam PFB139E is a Flame Retardant Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding Resin (also known as PFB1013Z590)Information provided by Eurostar. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
Ashley Polymers Ashlene® P1525B Polycarbonate A rigid flame retardant black polycarbonate, for applications requiring superior dimensional stability and overall toughness.Data provided by the manufacturer |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 113 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | Wet; ASTM D790 |
Asahi Kasei Leona® 54G43 43% Glass Filled Nylon 66 Enhanced strength, stiffness, and impact resistance; with 43% GF. Excellent appearance. Applications:Fans, railroad tie insulators, office furniture Information provided by Asahi Kasei |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | Dry; ASTM D790 |
Asahi Kasei Leona® CR301 Nylon 66 Suitable for a switch insulator. Low abrasion and superior electrical properties.Applications:Sliding switch insulators Information provided by Asahi Kasei |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | dry; ISO 178 |
DSM Novamid® 1013PL1 NAT PA6-MX Injection Molding |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | At 2 mm/min; ISO 178 |
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound Xmod K65G3 is a 30% glass fiber reinforced grade intended for injection molding. Xmod K65G3 has been developed especially for the car industry, to be used UTB parts. Xmod K65G3 offers good balance.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
PolyOne Lubri-Tech™ MP-30GF/15T Modified PPO - 30% Glass Fiber - 15% PTFE