Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.90 GPa | 566 ksi | STN EN ISO 178 |
Plastcom PLASTAMID® 66 GF 15 T 15 TS PA66 reinforced with glass fibers and mineral filler, heat stabilized Black PA66 for injection molding, reinforced with 15% glass fiber and 15% mineral filler, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of elect.. |
|||
Flexural Modulus | 3.90 GPa @Temperature 23.0 °C |
566 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYblend 65 M10 PC/ABS-blend, Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.90 GPa @Temperature 23.0 °C |
566 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T15040CR Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
Nilit FRIANYL B63 KV40 Nylon 6 for injection molding, 40% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC (Asia Pacific) LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
Nilit FRIANYL A63 BR80 Nylon 6.6 for injection molding, 80% bronze filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.90 GPa @Temperature 23.0 °C |
566 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 90P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact complian.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
M. Holland Company SA311 Styrene Acrylonitrile Medium clarityGood processabilityHigh stiffnessApplications: AppliancesCosmeticsHousehold goods |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
LG Chemical LUCEL MR-310 Low Warpage POM, 10% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON PD000 PA 6 (Europe-Africa-Middle East) LNP* STAT-KON* PD000 is a compound based on PA 6 resin containing Carbon Powder. Added features include: Electrically Conductive. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DFZ22P PC (Asia Pacific) LNP* THERMOCOMP* DFZ22P is a compound based on Polycarbonate resin containing Glass Fiber, Milled Glass. Added features of this material include: Exceptional Processing. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66 NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AW00A ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* AW00A is a compound based on Acrylonitrile Butadiene Styrene resin containing Wollastonite. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DFZ22P PC LNP THERMOCOMP* DFZ22P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 10% Milled Glass. Added features of this material include: Exceptional Processing. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178-93 |
Wellman Wellamid® GFT1699-WBK1 13% Glass Fiber Reinforced, Weatherable Black Nylon 66 Description: Glass Fiber Reinforced, Weatherable Black Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
Cresset Powers Cress-Alon™ NF3020 2% Nano Clay Loaded, 3.0 r.v. Film Grade Nylon 6, Dry As Molded Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
Clariant ABS4500G10BK ABS, 10% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 621 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 512 Polycarbonate, Glass Fiber/PTFE, UL Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 221 ABS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 3.90 GPa @Temperature 23.0 °C |
566 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYabs F00 GF17 ABS, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D 790 |
Saint-Gobain Meldin® 2021 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH303G20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH303G20 is a 20% glass filled Polypropylene - Homopolymer injection molding grade with good stiffness.Information provided by SAX Polymers |