Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.35 GPa | 341 ksi | ASTM D790 |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY XP4025 ASA (Europe-Africa-Middle East) GELOY XP4025 is a high heat modified ASA/PC blend, for automotive exterior applications. It shows very good properties, gloss and colour retention, as well as faster cycle time over competitive mate.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ISO 178 |
Radici Radilon® SHS (dry) Nylon 6 General PurposeInformation provided by Radici group. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HP2REU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a h.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
Flexural Modulus | 2.35 GPa @Thickness 6.40 mm |
341 ksi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Flexural Modulus | 2.35 GPa @Thickness 3.20 mm |
341 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR474F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ASTM D790 |
KKPC Kuhmo HFH 405 Flame Retarded HIPS Key features: Non-halogen type. Common Uses: Parts needing non-halogen type.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ASTM D790 |
Gromax CCP PBT 1100-600S Product Description: PBT unreinforced high viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excell.. |
|||
Flexural Modulus | 2.35 GPa @Thickness 3.20 mm |
341 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WX95752L PBT (Asia Pacific) LNP* Lubricomp* WX95752L is a compound based on Polybutylene Terephalate resin. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2mm/min; ISO 178 |
Teijin Panlite® L-1225L Standard (mold release/ice color grade) Polycarbonate Resin Thin-wall injection moldings grade of high fluidity. It has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:Comparatively large-size components of mechanic.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® UF-1017B PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ASTM Test |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ASTM D790 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Europe-Africa-Middle East) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ASTM D790 |
TPI Porene® GA800TW High Gloss/Weather Resistant/Antistatic Grade ABS INJECTION MOLDING; ANTISTATIC; WEATHER RESISTANT. HOUSING OF ELECTRICAL APPLIANCES, e.g. ELECTRIC FAN, TELEPHONE, CALCULATOR, TOYSPorene® is a registered trademark of Thai Petrochemical Industry C.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ASTM D790 |
Eastman Eastar EN076 Copolyester Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o.. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2 mm/min; ISO 178 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Flexural Modulus | 2.35 GPa @Thickness 6.40 mm |
341 ksi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Flexural Modulus | 2.35 GPa @Thickness 6.40 mm |
341 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM21M ABS Injection Molding Grade Medium Flow, Medium Impact, Medium RigidityInformation provided by Bhansali |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 2 mm/min; ISO 178 |
Covestro Makrolon® LED2643 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, .. |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® 500H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Flexural Modulus | 2.35 GPa | 341 ksi | ISO 178 |
Polyplastics Duracon® M25-45 Acetal Co-polymer (POM), Weather resistance, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |