Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 341 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 2.35 GPa
341 ksi
ASTM D790
Polimeri Europa Sinkral® PD L 322 ABS Resin
Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and..
Flexural Modulus 2.35 GPa
341 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East)
Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 2.35 GPa
341 ksi
ISO 178
Radici Radilon® S40E (dry) Nylon 6
High viscosity for extrusionInformation provided by Radici group.
Flexural Modulus 2.35 GPa
341 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer
Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin..
Flexural Modulus 2.35 GPa
341 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Asia Pacific)
Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin..
Flexural Modulus 2.35 GPa
341 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific)
LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci..
Flexural Modulus 2.35 GPa
341 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HP2REU PC (Europe-Africa-Middle East)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a h..
Flexural Modulus 2.35 GPa
341 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Europe-Africa-Middle East)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Flexural Modulus 2.35 GPa
341 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HPXS8R PC Copolymer
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Flexural Modulus 2.35 GPa
341 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Asia Pacific)
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Flexural Modulus 2.35 GPa
341 ksi
ISO 178
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy
Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago
Flexural Modulus 2.35 GPa
341 ksi
Mitsui AURUM® JNF3020 Thermoplastic Polyimide Resin, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Flexural Modulus 2.35 GPa
<br>@Thickness 6.40 mm
341 ksi
<br>@Thickness 0.252 in
15 mm/min; ASTM D790
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow
Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information ..
Flexural Modulus 2.35 GPa
341 ksi
2mm/min; ASTM D790
Kingfa JH950-502 Low-temperature Resistant & Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesGood low temperature resistanceGood normal/low temperature impact strengthGood surfaceApplications:ControllerPlugSocketShell of ammeterInformation ..
Flexural Modulus 2.35 GPa
341 ksi
ASTM D790
Kolon KOCETAL® K200 Standard Grade Acetal Resin
Suitable for both injection and extrusion.Applications: Injection and extruded use such as rod and sheetInformation provided by API Kolon.
Flexural Modulus 2.35 GPa
<br>@Thickness 3.20 mm
341 ksi
<br>@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY GP1000L PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical
Flexural Modulus 2.35 GPa
341 ksi
ASTM D790
GRECO ISOPAK 547 ABS Resin
High Impact GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Flexural Modulus 2.35 GPa
<br>@Temperature 23.0 °C
341 ksi
<br>@Temperature 73.4 °F
ASTM D790
IRPC Polimaxx Porene GA800 Acrylonitrile Butadiene Styrene
Applications:injection moldinghousing of electrical appliances such as electric fans, telephones, calculators and toys
Flexural Modulus 2.35 GPa
<br>@Thickness 3.20 mm
341 ksi
<br>@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Flexural Modulus 2.35 GPa
341 ksi
2mm/min; ISO 178
Teijin Panlite® LV-2225Y Standard (mold release/ice color grade) Polycarbonate Resin
Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required to be slightly high fluidity.Appl..
Flexural Modulus 2.35 GPa
341 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Modulus 2.35 GPa
341 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® LX-0971 S ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Flexural Modulus 2.35 GPa
341 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® NH-0700FX ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 2.35 GPa
341 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 2.35 GPa
341 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL N190X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications.
Flexural Modulus 2.35 GPa
341 ksi
ASTM D790
TPI Porene® KU900 Super High Heat ABS
INJECTION MOLDING. ELECTRICAL PARTS, AUTOMOTIVE APPLICATIONS, HOUSEHOLD GOODS, TOYSPorene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymer..
Flexural Modulus 2.35 GPa
341 ksi
ISO 178
Polyram RamTough PZ780 Polycarbonate, UV Stabilized
General purpose, UV stabilized polycarbonate for injection molding applications.Information provided by Polyram.
Flexural Modulus 2.35 GPa
341 ksi
2 mm/min; ISO 178
Covestro Makrolon® 2405 MAS048 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Flexural Modulus 2.35 GPa
341 ksi
2 mm/min; ISO 178
Covestro Makrolon® 2408 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Flexural Modulus 2.35 GPa
341 ksi
23°C, 50% RH; ASTM D790
Asahi Kasei Xyron® 500H Modified Polyphenylene Ether
Heat ResistantInformation provided by Asahi Kasei
Copyright © lookpolymers.com All Rights Reserved