Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.06 g/cc | 1.06 g/cc | 23°C; ASTM D792 |
Moisture Absorption | 0.0600 % | 0.0600 % | 23°C, 50% RH 24 hours; ASTM D570 |
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 49.0 MPa | 7110 psi | 23°C, 50% RH; ASTM D638 |
Elongation at Break | 50 % | 50 % | 23°C, 50% RH; ASTM D638 |
Flexural Strength | 83.0 MPa | 12000 psi | 23°C, 50% RH; ASTM D790 |
Flexural Modulus | 2.35 GPa | 341 ksi | 23°C, 50% RH; ASTM D790 |
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
2.16 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.05 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 70.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
38.9 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 120 °C | 248 °F | ASTM D648 |
Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
|
HB @Thickness 3.20 mm |
HB @Thickness 0.126 in |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | 50% RH; ASTM D257 |
Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | 50% RH; ASTM D257 |
Dielectric Constant | 2.8 @Frequency 1e+6 Hz |
2.8 @Frequency 1e+6 Hz |
50% RH; ASTM D150 |
2.8 @Frequency 1e+6 Hz |
2.8 @Frequency 1e+6 Hz |
50% RH; ASTM D150 | |
Dielectric Strength | 30.0 kV/mm @Thickness 2.00 mm |
762 kV/in @Thickness 0.0787 in |
Short time; ASTM D149 |
Dissipation Factor | 0.00050 @Frequency 60 Hz |
0.00050 @Frequency 60 Hz |
50% RH; ASTM D150 |
0.00060 @Frequency 1e+6 Hz |
0.00060 @Frequency 1e+6 Hz |
50% RH; ASTM D150 | |
Arc Resistance | 80 sec | 80 sec | Tungsten; ASTM D495 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 240 - 290 °C | 464 - 554 °F | Resin Temperature |
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
Drying Temperature | 90.0 - 100 °C | 194 - 212 °F | Pre-drying Temperature |
Dry Time | 2 - 4 hour | 2 - 4 hour |