Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 18.0 GPa | 2610 ksi | |
Plastcom SLOVAMID 6 GF 60 000/1M PA6 reinforced with 60% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 60% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ASTM D790 |
PolyOne Edgetek® XP9242701 Polyphenylene Sulfide (PPS) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3 sec Cycle Time: 18 to 70 secInformation provided by PolyOne |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | |
Plastcom SLOVAMID 6/66 CF 30 PA6/66, 30% carbon fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 30% of carbon fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-.. |
|||
Flexural Modulus | 18.0 - 22.0 GPa | 2610 - 3190 ksi | Injection; ISO 178 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | |
Cookson Group Plaskon® 150.401 Encapsulation Resin
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A second generation SMT-B family product. This material is the initial developmental, general purpose SMT-B encapsulation grade .. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1105-8529 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1-0784 Polyamide 66, with glass fiber and carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1105/XCF/20 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | |
Lehmann & Voss LUVOCOM® 1/XCF/25 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-190BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ASTM D790 |
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ASTM D790 |
Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced Applications: HousingsBracketsGear casesFeatures: High RigidityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | |
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ISO 178 |
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame.. |
|||
Flexural Modulus | >= 18.0 GPa | >= 2610 ksi | IEC 1212-2 5.2 |
Hippe PF WV 303 Wood veneer Reinforced Phenolic Resin - Sheet Parallel plied. Used in mechanical applications. Good mechanical properties.Information provided by Hippe. |
|||
Flexural Modulus | >= 18.0 GPa | >= 2610 ksi | IEC 1212-2 5.2 |
Hippe PF WV 304 Wood veneer Reinforced Phenolic Resin - Sheet Parallel plied. Used in mechanical and electrical applications.Information provided by Hippe. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ASTM D790 |
A. Schulman ComAlloy E-16026N Internally Lubricated, Carbon Fiber Reinforced Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ASTM D790 |
Gharda Chemicals GATONE™ 5330CF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ASTM D790 |
LATI LARTON GCE/60 60% Mixed Glass Fiber and Special Mineral Filled Polyphenylene sulfide (PPS)
(discontinued Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |
|||
Flexural Modulus | 18.0 GPa | 2610 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, Dry As Molded
  AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is rela.. |