| Category | Polymer , Thermoplastic , Polyphthalamide (PPA) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP VERTON |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP VERTON UX03320 PPA.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
| 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 | |
| Moisture Absorption | 0.200 % | 0.200 % | 50% RH, 24 hrs; ASTM D570 |
| 0.300 % | 0.300 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
| 0.00050 - 0.0010 cm/cm @Time 86400 sec |
0.00050 - 0.0010 in/in @Time 24.0 hour |
ASTM D955 | |
| Linear Mold Shrinkage, Transverse | 0.00080 - 0.0020 cm/cm @Time 86400 sec |
0.00080 - 0.0020 in/in @Time 24.0 hour |
ASTM D955 |
| 0.0015 cm/cm @Time 86400 sec |
0.0015 in/in @Time 24.0 hour |
ISO 294 | |
| Spiral Flow | 30.0 cm @Thickness 1.00 mm |
11.8 in @Thickness 0.0394 in |
SABIC Method |
| 70.0 cm @Thickness 3.00 mm |
27.6 in @Thickness 0.118 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 200 MPa | 29000 psi | ISO 527 |
| 220 MPa | 31900 psi | ASTM D638 | |
| Elongation at Break | 1.9 % | 1.9 % | ASTM D638 |
| 1.9 % | 1.9 % | ISO 527 | |
| Tensile Modulus | 18.2 GPa | 2640 ksi | 5 mm/min; ASTM D638 |
| 20.3 GPa | 2940 ksi | 1 mm/min; ISO 527 | |
| Flexural Strength | 300 MPa | 43500 psi | ASTM D790 |
| 360 MPa | 52200 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 17.7 GPa | 2570 ksi | 2 mm/min; ISO 178 |
| 18.0 GPa | 2610 ksi | ASTM D790 | |
| Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Impact Test | 19.0 J | 14.0 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 12.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
6.67 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 12.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
6.67 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 275 °C | 527 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 260 °C @Thickness 3.20 mm |
500 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Flammability, UL94 | HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
UL 94 |