Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.18 GPa | 1040 ksi | ASTM D790 |
PolyOne Stat-Tech™ CTX-1125 Natural Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
Shell Carilon® DP R1130 Polyketone, 30% Glass Fiber Reinforced
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1130 is a 30 percent glass fiber reinforced compound based on a developmental e.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178 |
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | |
Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | |
Lehmann & Voss Nylatron® MR 2007 Polyamide 6, with mineral filler Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Flexural Modulus | 7.15 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Flexural Modulus | 7.15 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East) High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East) 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Flexural Modulus | 7.15 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East) DATA ON BK1005 ONLY. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific) DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RFZ349 PA 66 (Asia Pacific) LNP* Thermocomp* RFZ349 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WFB44 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WFB44 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Glass Bead. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Asia Pacific) PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump .. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178 |
Solvay TECHNYL® AR 218 V25 Nylon 66, 25% glass fiber, DRY Description: Polyamide PA66 reinforced with 25% of glass fiber, heat stabilized, containing recycled material.Available in: Europe and North AmericaProduct Applications: TECHNYL® AR 218 V25 BLACK.. |
|||
Flexural Modulus | 7.15 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend High flow Ultem for thin wall application |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp EF006R PEI (Europe-Africa-Middle East) LNP* Thermocomp* EF006R is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Mold Release.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
Plenco 7507 Phenolic, Granular, Injection Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide AG5 PA66, 25% Glass Filled, Injection Molded AG5 is a 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
E-Polymers Tekaloy® G70GR , 30% Glass Reinforced PC/ABS Alloy 30% Glass Fiber reinforced, High stiffness, Dimensional stabilityInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
E-Polymers TEKAMID® TA210M40 , 40% Mineral Filled PA66, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
Chem Polymer Chemlon 125-15 MG Nylon 66, 25% Mineral/15% Glass Fiber Reinforced A 25% mineral reinforced, 15% glass fiber reinforced nylon 66 offering excellent rigidity, dimensional stability and tensile strength with improved warpage control in large area parts.Data provided .. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
Ashley Polymers Ashlene® 520-33GU Nylon 66, 33% Glass Reinforced Nylon 66, 33% glass reinforced resin, utility grade for non-critical applications. Also available: 520S - 33GU Heat Stabilized, 520 - 33GBU Black, 520S - 33GBU Black with H.S.Data provided by the m.. |
|||
Flexural Modulus | 7.17 GPa @Temperature 100 °C |
1040 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
Flexural Modulus | 7.16 GPa | 1040 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON QE002S PA6.10 LNP* STAT-KON* QE002S is a compound based on Nylon 6/10 containing 10% carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive. |