Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T8038 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYsan PN127 Styrene Acrylonitrile Information provided by Polykemi AB |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and .. |
|||
Flexural Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYabs F00 GF15 ABS, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PP HIP8040F VT2 Polypropylene, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
Panjin Zhongrun Chemerize 012G High Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Flexural Modulus | 3.70 - 9.50 GPa | 537 - 1380 ksi | Average value: 7.89 GPa Grade Count:23 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 2mm/min; ASTM D790 |
Kingfa JH960 6610 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
Mitsubishi Xantar® MX 1081 Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | |
Haysite HTF Polyester, High Temp Flex HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
IRPC Polimaxx Polene 1111NX TA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 20% TALCUM REINFORCEDAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Dry Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-810 Polyetheretherketone (PEEK) KetaSpire® KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0.50 kPa-s for standard high-viscosity PEEK grades .. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-810FP Polyetheretherketone (PEEK) KetaSpire® KT-810FP is the fine powder form of KT-810 resin. KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DFD029 PC (Europe-Africa-Middle East) LNP* Stat-kon* DFD029 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Reta.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX05477 PC LNP THERMOCOMP* DX05477 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 3 points and 2 mm/min; ISO 178 |
Styron Pulse® 979 PC/ABS PULSE™ 979 is a high performance, 10% glass filled PC/ABS resin.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RB004 PA 66 LNP* THERMOCOMP* RB004 is a compound based on Nylon 66 containing Glass Beads. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM-D790 |
Polyram RamTough PZ307G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced, UV stabilized polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | ASTM D 790 |
Cossa Polimeri ESTASAN SAN 3000 Styrene Acrylonitrile High melt flow rate, good chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 3.70 GPa | 537 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GS 25 HWCP 25% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |