Material Notes:
HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high temperature is required. Standard color is tan. Thickness is 1/32" - 1/16". Sheet sizes are 36" x 72" and 48" x 96".Information provided by Haysite
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Water Absorption 1.1 %
1.1 %
ASTM D229
Mechanical Properties Metric English Comments
Hardness, Barcol 16
16
Tensile Strength 42.7 MPa
6200 psi
LW; ASTM D638
46.2 MPa
6700 psi
CW; ASTM D638
Tensile Strength, Ultimate 52.0 MPa
7540 psi
Flexural Strength 83.0 MPa
12000 psi
Flexural Modulus 3.70 GPa
537 ksi
Compressive Strength 74.5 MPa
10800 psi
Flatwise; ASTM D695
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
Edgewise (CW); ASTM D256
5.34 J/cm
10.0 ft-lb/in
Edgewise (LW); ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Approximate temperature class
200 °C
392 °F
Elec.
200 °C
392 °F
Mech.
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 5.2

@Frequency 60.0 Hz
5.2

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm
560 kV/in
Perpendicular in Air; ASTM D149
23.6 kV/mm
600 kV/in
Perpendicular in Oil; ASTM D149
Dielectric Breakdown 55000 V
55000 V
Parallel, Step-By-Step in Oil; ASTM D149
Dissipation Factor 0.057

@Frequency 60.0 Hz
0.057

@Frequency 60.0 Hz
ASTM D150
Arc Resistance 135 sec
135 sec
ASTM D495