Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.60 GPa | 377 ksi | STN EN ISO 178 |
Plastcom PLASTAMID® 6 BT N 32 B PA6 Basic type PA 6 for compounding, for general use. Delivered in the natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | Tangent; 1.3 mm/min; ASTM D790 |
Mytex Polymers AX1166 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: InteriorInformation provided by Mytex Polymers |
|||
Flexural Modulus | 2.60 GPa @Temperature 23.0 °C |
377 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | ISO 178 |
Radici Radilon® ALX14080 (dry) Nylon 66 Medium high viscosityInformation provided by Radici group. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, Dry As Molded
(discontinued **) AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resist.. |
|||
Flexural Modulus | 2.60 GPa @Temperature 23.0 °C |
377 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYform POM C M90 Polyoxymethylene Information provided by Polykemi AB |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
Nilit Polynil® P60 Medium Viscosity Nylon 66 Description: Polynil P60 is a grade has a viscosity that has been optimized for monofilament extrusion.Key characteristics: Viscosity number 155 gr/cm3Excellent melt stabilityHigh elongationInformat.. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
Ineos Nova 1552 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Easy processing, High modulus, Improve stress whitening, Custom colorsApplications: Injection molding, Office furniture, Electronic media, Photographic equipmentPerformance grades of polystyrene are.. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Asia Pacific) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
LG Chemical LUCEL VC127-LD Antistatic POM, Unreinforced, High Flow, For VCR Reels LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | |
Aardvark Polymers AARTEL® 820UV Acetal Copolymer Rotational Molding Resin Aartel 820UV is a natural acetal copolymer with added UV stabilizers.Aartel 820UV is a low viscosity resin with excellent flow characteristics.Aartel 820UV is available in natural white and may be p.. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | |
Lehmann & Voss LUVOCOM® 1100-7337/WT Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC (Asia Pacific) LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.60 GPa @Temperature 23.0 °C |
377 ksi @Temperature 73.4 °F |
2mm/min; 80x10x4mm; ISO 178 |
SYNTHOS Forsan® 393 Acrylonitrile Butadiene Styrene (ABS) High heat resistance, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Ka.. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX1007 PPE+PS Noryl* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A.. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | ASTM-D790 |
Polyram PlusTek PB801 Nylon 6, Impact Modified impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | dry; ISO 178 |
DSM Akulon® F-X9183 PA6 Low/Medium Viscosity |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | dry; ISO 178 |
DSM Akulon® K125/A PA6 Low Viscosity |
|||
Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
Ashley Polymers Ashlene® 195-N2 Acetal A general purpose, medium viscosity natural.Data provided by the manufacturer |
|||
Flexural Modulus | 2.60 GPa @Temperature 23.0 °C |
377 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH TS15030 D Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |