Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Plaskolite Vivak PETG Sheet VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details... |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | Tangent; ASTM D790 |
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | Tangent; ASTM D790 |
RheTech Products HP531-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: IP structural componentsAir ducts - distributionA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D 790 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate Information provided by Ravago. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | Tangent; ASTM D790 |
RheTech Products HP531-679UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, 2B5A Black Ink Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | Tangent; ASTM D790 |
RheTech Products M25P251-01 25% Mica Reinforced Polypropylene Copolymer, Black Applications: Fan shroudsGlove box binFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | initial |
Malvern Minerals Nylon with Novacite® L-337 Quartz Filler Product data demonstrates the effect of the Novacite® (untreated lamellar quartz) filler. A separate entry demonstrates the effect of treated Novakup® filler in nylon. The specific nylon use.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Global ABS-FR0 High Impact, Flame Resistant ABS Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Global HI-830 High Impact Polystyrene High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys |
|||
Flexural Modulus | 2.14 GPa @Temperature 23.0 °C |
310 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene HI830 Polystyrene APPLICATIONS: EXTRUSION APPLICATION, VACUUM SHEET : FOOD PACKAGING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY, etc. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Techmer ES HiFill FR® ASA FR-2 WT Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Spartech 829 Static Conductive Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Spartech Korad® SP-9071 FR/ABS Flame Retardant Sheet Description: Flame Retardant SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | secant; ASTM D790 |
Spartech PP5130 Talc Filled Homopolymer Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Spartech SP-9030 Economy ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Flexural Modulus | 2.14 GPa @Thickness 3.17 mm |
310 ksi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.14 GPa @Thickness 3.17 mm |
310 ksi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.14 GPa @Thickness 3.17 mm |
310 ksi @Thickness 0.125 in |
|
TPI Porene® ABS-AN450 Flame Retardant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Total PSI 945 Polystyrene Polystyrene 945 is designed for injection molding applications requiring superior toughness. This polymer is a high impact polystyrene with excellent gloss and falling dart properties. The impact an.. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Aaron Industries AAROPRENE® TFIPP 2020 High Impact Talc Filled Polypropylene AAROPRENE® TFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-10FG-0100 10% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Proto3000 PC ISO Fused Deposition Modeling Polymer Description: PC-ISO (polycarbonate-ISO), an industrial thermoplastic, which in its raw state, meets the ISO 10993-1 and USP Class VI classi?cation 1. PC-ISO blends are commonly used in food and drug.. |
|||
Flexural Modulus | 2.14 GPa @Temperature 23.0 °C |
310 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Porene AN520 Acrylonitrile Butadiene Styrene Applications:injection moldingelectrical appliances such as microwaves, computers, tv, switch boxes, switch panels, etc.automotive componenets |
|||
Flexural Modulus | 2.14 GPa | 310 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |