Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IRPC Polimaxx Porene AN520 Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer IRPC Polimaxx
Trade Name Porene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Porene AN520 Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications:injection moldingelectrical appliances such as microwaves, computers, tv, switch boxes, switch panels, etc.automotive componenets
Physical Properties Metric English Comments
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107

@Thickness 6.35 mm,
Temperature 23.0 °C
107

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D785
Tensile Strength, Ultimate 42.2 MPa

@Temperature 23.0 °C
6120 psi

@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength 56.4 MPa

@Temperature 23.0 °C
8180 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 2.14 GPa

@Temperature 23.0 °C
310 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 0.883 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.65 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C

@Thickness 6.35 mm
180 °F

@Thickness 0.250 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C

@Thickness 6.35 mm
167 °F

@Thickness 0.250 in
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Users viewing this material also viewed the following: