Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
Multibase Multi-Pro® 2510 XGW Polypropylene Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 1.37 - 2.76 GPa | 199 - 400 ksi | Average value: 2.09 GPa Grade Count:36 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Flexural Modulus | 1.37 GPa | 198 ksi | 12.5 mm/min; ASTM D790 |
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade
(discontinued **) ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo.. |
|||
Flexural Modulus | 1.37 GPa | 198 ksi | ASTM D790 |
LyondellBasell Moplen HP400H Polypropylene Homopolymer Description: Moplen HP400H is a homopolymer for extrusion applications. Moplen HP400H exhibits easy processability and a good stiffness/impact balance at ambient temperature. The main applications .. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
Hyosung Topilene F300 PP F300 Film Grade HomopolymerApplications: OPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
Hyosung Topilene HB240P PP HB240P Applications:Industrial pipesSewerage pipesCharacteristics:High impact strengthHigh ring stiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
Hyosung Topilene HJ746 PP HJ746 Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | 1% Secant; ASTM D790 |
Flint Hills P4G4T-017A Homopolymer Polypropylene Homopolymer, and FDA compliant.Features: Highly lubricated and antistat.Applications: Injection molding: closures.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Flexural Modulus | 1.37 GPa @Thickness 3.20 mm |
199 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HI100X ABS, High Impact, Semi-Transparency, Flexible Feature: Injection Molding, High Impact, Semi-Transparency, FlexibleApplication: Artificial Nails, Miscellaneous Goods)CAS No. 9010-94-0Information provided by LG Chemical |
|||
Flexural Modulus | 1.37 GPa @Thickness 6.40 mm |
199 ksi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL HG3100 PP+MF10%, High Gloss Description: Injection Molding, PP+MF10%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | 15mm/min; ASTM D790 |
LG Chemical LUTENE-H BE0400 HDPE Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.Applications: Blow molded con.. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® PM200 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP (Asia Pacific) LNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized, Low Extractible. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific) LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific) LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP High modulus/impact/heat PPE+PP |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP (Asia Pacific) High modulus/impact/heat PPE+PP. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX7115F PPE+PP High modulus/impact/heat PPE+PP. Compliant with US FDA food contact regulations for temperatures of use of room temperature and below. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H6240B High Density Polyethylene Blow Molding Key Characteristics:Good stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthGood appearanceOdorlessSafe for food contactGood printabilityRecommended App.. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P642J Polypropylene Injection Molding Key Characteristics:Good flowabilityExcellent stiffnessHigh impact strengthMechanical property balanceContains UV stabilizer and anti-static agentRecommended Applications:Industrial and household pr.. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
Tipco Tipcolene® FX 4000 - UL94-V0 Flame Retardant Polypropylene Copolymer, High Impact Strength V-0 Flame Retardant PP Copolymer with High Impact StrengthApplications: Battery HousingsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
Tipco Tipcolene® FX 4002 - UL94-V2 Flame Retardant Polypropylene Copolymer Compound with High Impact Strength V-2 Flame Retardant PP Copolymer with High Impact StrengthApplications: Battery LidsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | ASTM D790 |
Tipco Tipcolene® PP-LTHA - Unfilled Polypropylene Homopolymer with Long Term Heat Aging Stability PP Homopolymer with Long Term Heat Aging StabilityApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 1.37 GPa | 199 ksi | Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
Chevron Phillips Marlex® HHM 5502LW Polyethylene; HDPE High density polyethylene. This high molecular weight, hexene copolymer with synthetic antistatic agent is tailored for lightweight blow molded containers that: Require excellent stiffnessRequire .. |