| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0070 cm/cm <br>@Thickness 3.20 mm |
0.0060 - 0.0070 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.0080 cm/cm <br>@Thickness 3.20 mm |
0.0060 - 0.0080 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Melt Flow | 14 g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C |
14 g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 34.0 MPa | 4930 psi | Type I, 50 mm/min; ASTM D638 |
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | Type I, 50 mm/min; ASTM D638 |
| Elongation at Break | 125 % | 125 % | Type I, 50 mm/min; ASTM D638 |
| Elongation at Yield | 8.0 % | 8.0 % | Type I, 50 mm/min; ASTM D638 |
| Tensile Modulus | 1.24 GPa | 180 ksi | 50 mm/min; ASTM D638 |
| Flexural Yield Strength | 51.0 MPa | 7400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 1.37 GPa | 199 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
| Dart Drop, Total Energy | 37.0 J <br>@Temperature 23.0 °C |
27.3 ft-lb <br>@Temperature 73.4 °F |
ASTM D3763 |
| 44.0 J <br>@Temperature -30.0 °C |
32.5 ft-lb <br>@Temperature -22.0 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 162 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
90.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| CTE, linear, Transverse to Flow | 97.2 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
54.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 112 °C <br>@Thickness 3.20 mm |
234 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 85.0 °C <br>@Thickness 3.20 mm |
185 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |