Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® HHM 5502LW Polyethylene; HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HHM 5502LW Polyethylene; HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High density polyethylene. This high molecular weight, hexene copolymer with synthetic antistatic agent is tailored for lightweight blow molded containers that: Require excellent stiffnessRequire exceptional processabilityAre durable and recyclable for sustainabilityApplications: Typical blow molded applications for HHM 5502LW include: Detergent bottlesHousehold and industrial chemical containersPharmaceuticalsInformation provided by PhillipsThis resin meets these specifications: ASTM D4976 – PE 235FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c)Listed in the Drug Master File
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D-1505
ESCR 100% Igepal® 30 hour
30 hour
Condition B, F50; ASTM D-1693
Melt Index of Compound 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
2 in/min, Type IV bar; ASTM D-638
Elongation at Break 500 %
500 %
2 in/min, Type IV bar; ASTM D-638
Flexural Modulus 1.37 GPa
199 ksi
Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
Type A, Type I specimen; ASTM D-746
Users viewing this material also viewed the following: