Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 62.0 - 100 MPa | 8990 - 14500 psi | Average value: 93.8 MPa Grade Count:7 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | 15.0 - 100 MPa | 2180 - 14500 psi | Average value: 71.3 MPa Grade Count:141 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Strength, Ultimate | 80.0 - 100 MPa | 11600 - 14500 psi | ASTM D638 |
Chang Chun Plastic PBT3015 15% Glass Fiber Enforced PBT Information provided by Dowell Trading Company Ltd. |
|||
Tensile Strength, Ultimate | 40.0 - 100 MPa @Temperature -40.0 - 80.0 °C |
5800 - 14500 psi @Temperature -40.0 - 176 °F |
Average value: 71.0 MPa Grade Count:1 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Tensile Strength, Ultimate | 82.7 - 100 MPa | 12000 - 14500 psi | Average value: 91.9 MPa Grade Count:7 |
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Tensile Strength, Ultimate | 35.0 - 100 MPa @Temperature -40.0 - 70.0 °C |
5080 - 14500 psi @Temperature -40.0 - 158 °F |
Average value: 67.5 MPa Grade Count:4 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Ultimate | 33.0 - 100 MPa | 4790 - 14500 psi | Average value: 47.4 MPa Grade Count:29 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Tensile Strength, Ultimate | 10.0 - 100 MPa @Temperature -20.0 - 100 °C |
1450 - 14500 psi @Temperature -4.00 - 212 °F |
Average value: 45.0 MPa Grade Count:2 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Ultimate | 10.0 - 100 MPa @Strain 1.00 - 8.00 % |
1450 - 14500 psi @Strain 1.00 - 8.00 % |
Average value: 45.0 MPa Grade Count:2 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Ultimate | 70.0 - 100 MPa @Temperature -40.0 - -40.0 °C |
10200 - 14500 psi @Temperature -40.0 - -40.0 °F |
Average value: 85.0 MPa Grade Count:4 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |