Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® EM2212 PC Automotive interiors. 10% glass-reinforced. Increased stiffness/structural ridigity. High modulus/ductile. Foamed skin instrument panel uses also. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763 |
LyondellBasell Hifaxâ„¢ HSBMG265 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ HSBMG265 medium high melt flow, 1,400 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of rigidity, .. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763 |
LyondellBasell Hifaxâ„¢ RTA3263EUV/1 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV/1 fractional melt flow, 1,700 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent b.. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
Instrumented Peak Energy; ASTM D3763 |
LyondellBasell Hostacomâ„¢ RE-44AC Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RE-44AC polypropylene TPO resin is a compounded product containing 25% minimum post-industrial or post-consumer recycled polypropylene and reactor grade thermoplastic ole.. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Asia Pacific) LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DZL24 PC LNP LUBRICOMP* DZL24 is a compound based on Polycarbonate resin containing 20% Milled Glass, 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS (Asia Pacific) Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DE003Z PC LNP STAT-KON* DE003Z is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Extrusion Grade. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON MD000IS PP LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific) LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP D351 PC (Asia Pacific) LNP* Thermocomp* D351 (experimental grade name as EXTC8143) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus,.. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: .. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific) 20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific) Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP EXTC8143 PC (Asia Pacific) LNP* Thermocomp* EXTC8143 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, No.. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing 45% Glass Fiber. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA (Asia Pacific) 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
Dart Drop, Total Energy | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DEP32 PC LNP* STAT-KON* DEP32 is a compound based on Polycarbonate containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 (Asia Pacific) LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Asia Pacific) LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
Dart Drop, Total Energy | 24.0 J @Temperature -15.0 °C |
17.7 ft-lb @Temperature 5.00 °F |
Instrumented, Energy at Maximum Load, Ductile Failure; ASTM D3763 |
LyondellBasell Hifax™ ETA3163/1 Thermoplastic Polyolefin Elastomer Description: Hifax™ ETA3163/1 medium melt flow, 900 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffness and low temper.. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL004XXC PC LNP* LUBRICOMP* DL004XXC is a compound based on Polycarbonate containing 20% PTFE. Characteristics of this grade are: Interrnally Lubricated. |
|||
Dart Drop, Total Energy | 24.0 J | 17.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |