Polymer Property : Flexural Yield Strength = 6960 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 48.0 MPa
6960 psi
ASTM D790
North Wood Plastics Polypropylene with 40% Wood Fiber, Molding Grade
Data provided by North Wood Plastics, Inc.
Flexural Yield Strength 48.0 MPa
6960 psi
ASTM D790
North Wood Plastics PS with 20% Wood Fiber
Data provided by North Wood Plastics, Inc.
Flexural Yield Strength 48.0 - 255 MPa
6960 - 37000 psi
Average value: 84.2 MPa Grade Count:104
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Flexural Yield Strength 48.0 MPa
6960 psi
ASTM D790
Ineos Nova 3900 General Purpose Crystal Polystyrene  (discontinued **)
High flow, Good compoundingApplications: Color concentrates, Compounding, Thin wall moldingsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and o..
Flexural Yield Strength 48.0 - 172 MPa
6960 - 24900 psi
Average value: 76.4 MPa Grade Count:15
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..
Flexural Yield Strength 48.0 MPa
6960 psi
ASTM D790
Ineos Nova 5400 High Impact Polystyrene
High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were..
Flexural Yield Strength 48.0 MPa
6960 psi
ASTM D790
Ineos Nova 5404 High Impact Polystyrene
High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were..
Flexural Yield Strength 48.0 MPa
6960 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer
Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity...
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Asia Pacific)
Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Europe-Africa-Middle East)
Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X6800BM PBT
Blow moldable, impact modifed XENOYThis data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific)
Blow moldable, impact modifed XENOY
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-LOY KX05015 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Stat-Loy* KX05015 is a compound based on Acetal Copolymer resin containing Antistat. Added features include permanent Anti-Static.
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-LOY KX09024 ACETAL COPOLYMER (Europe-Africa-Middle East)
LNP* Statloy* KX09024 is a compound based on Polyacetal with reduced Resistivity. Added features include: Antistatic Properties
Flexural Yield Strength 48.0 MPa
6960 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl HIPS3191 PS
This data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Europe-Africa-Middle East)
PPE+PP blend. Suitable for painted exterior automotive applications.
Flexural Yield Strength 48.0 MPa
6960 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Flexural Yield Strength 48.0 MPa
6960 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Flexural Yield Strength 48.0 MPa
6960 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Flexural Yield Strength 48.0 MPa
6960 psi
ASTM D790
Washington Penn H2GF3 Polypropylene, 30% Glass Fiber Reinforced
Homopolymer. Excellent heat aged physical properties.Applications: Under hood applications, battery trays, exercise equipmentData provided by Washington Penn Plastic Co., Inc.
Flexural Yield Strength 48.0 - 55.0 MPa
6960 - 7980 psi
ASTM D790
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Flexural Yield Strength 48.0 MPa
6960 psi
ASTM D790
Ineos Nova 5450 High Impact Polystyrene  (discontinued **)
High impact, Good ESCRApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were determined on injection molded specimens at 23..
Flexural Yield Strength 48.0 MPa
6960 psi
ASTM D790
Ineos Nova 5500 High Impact Polystyrene  (discontinued **)
Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio..
Flexural Yield Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X6800BM PBT (Europe-Africa-Middle East)
Blow moldable, impact modifed XENOY
Flexural Yield Strength 48.0 MPa
6960 psi
ASTM D790
Ineos Nova 5504 High Impact Polystyrene  (discontinued **)
Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio..