Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | Xenoy® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
Moisture Absorption | 0.0100 % | 0.0100 % | 23°C / 50% RH; ISO 62 |
Water Absorption at Saturation | 0.10 % | 0.10 % | ISO 62 |
Linear Mold Shrinkage, Flow | 0.0285 - 0.0335 cm/cm @Thickness 3.20 mm |
0.0285 - 0.0335 in/in @Thickness 0.126 in |
SABIC Method |
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
Melt Index of Compound | 9.0 g/10 min @Load 5.00 kg, Temperature 265 °C |
9.0 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 38.0 MPa | 5510 psi | 50 mm/min; ISO 527 |
48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 | |
Tensile Strength, Yield | 31.0 MPa | 4500 psi | 50 mm/min; ISO 527 |
35.0 MPa | 5080 psi | Type I, 50 mm/min; ASTM D638 | |
Elongation at Break | 167 % | 167 % | 50 mm/min; ISO 527 |
238 % | 238 % | Type I, 50 mm/min; ASTM D638 | |
Elongation at Yield | 11 % | 11 % | Type I, 50 mm/min; ASTM D638 |
14.4 % | 14.4 % | 50 mm/min; ISO 527 | |
Tensile Modulus | 1.69 GPa | 245 ksi | 5 mm/min; ASTM D638 |
1.70 GPa | 247 ksi | 1 mm/min; ISO 527 | |
Flexural Yield Strength | 48.0 MPa | 6960 psi | 2 mm/min; ISO 178 |
51.0 MPa | 7400 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Flexural Modulus | 1.42 GPa | 206 ksi | 2 mm/min; ISO 178 |
1.65 GPa | 239 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Izod Impact, Notched | 8.02 J/cm | 15.0 ft-lb/in | ASTM D256 |
1.86 J/cm @Temperature -30.0 °C |
3.48 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
Izod Impact, Notched (ISO) | 95.0 kJ/m² | 45.2 ft-lb/in² | 80*10*4; ISO 180/1A |
22.0 kJ/m² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
Charpy Impact, Notched | 12.9 J/cm² | 61.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
CTE, linear, Transverse to Flow | 170 µm/m-°C @Temperature -40.0 - 40.0 °C |
94.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
170 µm/m-°C @Temperature -40.0 - 40.0 °C |
94.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
Deflection Temperature at 1.8 MPa (264 psi) | 46.0 °C | 115 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
47.0 °C @Thickness 3.20 mm |
117 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
Vicat Softening Point | 115 °C | 239 °F | Rate B/120; ISO 306 |
115 °C | 239 °F | Rate B/50; ASTM D1525 | |
118 °C | 244 °F | Rate B/50; ISO 306 |