Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min; ASTM D790 |
Ovation Polymers RIGITRON 10030 GF Polycarbonate, 30% Glass Reinforced PC - Glass reinforced (30 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared accor.. |
|||
Flexural Yield Strength | 140 - 240 MPa | 20300 - 34800 psi | Average value: 182 MPa Grade Count:6 |
Overview of materials for Phenolic, Resole, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | ASTM Data |
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | ASTM Data |
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resista.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | at 3.5% strain; Conditioned; ISO 178-A |
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). UL94 V0, V2 and 5VA listing. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1100R PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1110F PEI (Europe-Africa-Middle East) Enhanced flow PolyetherimiEnhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no long.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. RoHS compliant and UL94 V0 listed. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem MD130A PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant, ISO 10993 compliant in recognized colors.This data was supplied by SABIC-IP for the Europe-.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Asia Pacific) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX138H PPE+HIPS (Asia Pacific) Modified PPO Resin with 20% Glass Fibre Reinforced |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 9090 PEI Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | ISO 178 |
Wellman Wellamid® MR409 22H-N 40% Mineral Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | ASTM D790 |
E-Polymers TEKAMID® TB110M40 , 40% Mineral Filled PA6, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | ASTM D790 |
E-Polymers TEKANATE™ G715FR , Flame Retardant, 15% Glass Fiber Reinforced Poly Carbonate 15% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Yield Strength | 140 - 180 MPa | 20300 - 26100 psi | ASTM D790 |
Chang Chun Plastic PBT4115 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | ASTM Data |
BASF Capron® 8331G HS Blend Impact Modified, 14% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8331G HS Blend is a 14% glass fiber reinforced, heat stabilized, polyamide 6 molding compound developed for applications requiring improved toughness in combination with a balance of strength.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | ASTM Data |
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8333G HI is a 33% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance .. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 3412ECR PC Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |