Overview of materials for Phenolic, Resole, Glass Fiber Filled

Category Polymer , Thermoset , Phenolic , Phenolic, Resole, Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Phenolic, Resole, Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.70 - 1.90 g/cc
0.0614 - 0.0686 lb/in³
Average value: 1.78 g/cc Grade Count:6
Water Absorption 0.0400 - 0.350 %
0.0400 - 0.350 %
Average value: 0.170 % Grade Count:5
Linear Mold Shrinkage 0.00150 - 0.00300 cm/cm
0.00150 - 0.00300 in/in
Average value: 0.00213 cm/cm Grade Count:6
Mechanical Properties Metric English Comments
Hardness, Rockwell E 80.0 - 90.0
80.0 - 90.0
Average value: 85.0 Grade Count:4
Tensile Strength, Ultimate 50.0 - 125 MPa
7250 - 18100 psi
Average value: 90.5 MPa Grade Count:6
Flexural Yield Strength 140 - 240 MPa
20300 - 34800 psi
Average value: 182 MPa Grade Count:6
Flexural Modulus 13.8 - 17.0 GPa
2000 - 2470 ksi
Average value: 15.2 GPa Grade Count:6
Compressive Yield Strength 234 - 275 MPa
33900 - 39900 psi
Average value: 249 MPa Grade Count:6
Izod Impact, Notched 0.270 - 0.590 J/cm
0.506 - 1.11 ft-lb/in
Average value: 0.413 J/cm Grade Count:3
Charpy Impact, Notched 0.340 - 0.500 J/cm²
1.62 - 2.38 ft-lb/in²
Average value: 0.413 J/cm² Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 5.00 - 25.0 µm/m-°C
2.78 - 13.9 µin/in-°F
Average value: 15.0 µm/m-°C Grade Count:6
Thermal Conductivity 0.410 - 0.790 W/m-K
2.85 - 5.48 BTU-in/hr-ft²-°F
Average value: 0.583 W/m-K Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 155 - 282 °C
311 - 540 °F
Average value: 258 °C Grade Count:6
Electrical Properties Metric English Comments
Dielectric Strength 11.4 - 32.0 kV/mm
290 - 813 kV/in
Average value: 16.1 kV/mm Grade Count:5
Arc Resistance 135 - 180 sec
135 - 180 sec
Average value: 164 sec Grade Count:4