Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.20 GPa | 464 ksi | STN EN ISO 527-2 |
Plastcom PLASTAMID® 610 BT N 32 B PA610 Basic type PA610 for injection molding, modified for general use. Use: extrusion, filaments, injection molding. Delivered in the natural color.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Asia Pacific) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 |
Nilit FRIANYL B63 K Nylon 6 for injection molding Nylon 6 for injection molding, specially formulated for knobs.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Europe-Africa-Middle East) LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
Tensile Modulus | 3.20 GPa @Temperature 23.0 °C |
464 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers, pigmented red, having extremely low VOC emissions, developed for automotive interior applicatio.. |
|||
Tensile Modulus | 3.20 GPa @Temperature 23.0 °C |
464 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® FG400XRD NC010 Acetal
(Unverified Data**) Delrin® FG400XRD NC010 is a filled, medium viscosity acetal copolymer for injection molding. It is detected in x-ray detectors. It has been developed for consideration into applications such as par.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | Conditioned 50% RH; ISO 527 |
Manifattura Cattaneo PA 6.6 30% GF Nylon, Glass Filled Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-1,-2 |
Lanxess Durethan® B 40 SK 000000 Nylon 6 PA 6, non-reinforced, injection molding |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ASTM D638 |
Ineos ABS Lustran® SAN Sparkle Highest-Clarity |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 222 Black 1N PA66, DRY Description: Unreinforced polyamide PA66, medium viscosity, heat stabilized, for injection molding, fast crystallization, for short cycles .Available in: EuropeProduct Applications: TECHNYL A 222 of.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP PFP36 PA 6 (Asia Pacific) LNP* PFP36 is a compound based on Nylon 6 containing Glass Fiber and PTFE/Silicone. Characteristics are Impact Modifier. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 1010F PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010FV PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1mm/min; ISO 527-1, 2 |
Polyplastics TOPAS® 5013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) This grade is characterized by its high flowability and superior optical properties. It is suitable for optical components such as lenses and light guide panels where high molded precision is indisp.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ASTM-D790 |
Polyram PlusTek PB847I4 Nylon 6, 20% Glass Fiber and Mineral 20% glass fiber and mineral reinforced, impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | |
Hexcel® HexPly® F522 Epoxy Resin HexPly® F522 is an advanced, modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness, excellent hot-wet properties .. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527-1/-2 |
Covestro Bayblend® FR 3020 Polycarbonate + ABS, Mineral Filled 5 % mineral filledfor thin-wall applicationsinjection moldingVicat/B 120 = 103 °CHDT/A = 85 °Cvery good UL listing in small wall thickness (V-0 at 0.75 mm)PreprocessingMax. Water content |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 SUVCP Nylon 6, Finely Crystalline, UV Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWL UL-Licensed Nylon 66, Flame Protection Grade V-2, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ISO 527 |
Eurotec® Tecomid® NA40 NL E PA 6.6 lubricated, nucleated Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437G25M5CL Glass/Mineral Reinforced Coupled |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1mm/min; ISO 527 |
BASF Ultramid® A34 01 PA66 (Dry) Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or .. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | |
Parylene Coating Services C Poly (P-Xylylene) Monomer is monochloro para-xylylene. Parylene C is recommended where excellent barrier protection is needed. It can be used up to 125°C where oxygen is present.Parylene is a generic name for poly-.. |
|||
Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermotuf PK003EI2 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PK003EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include High Impact, Easy Molding.This data was supplied by SABIC-IP for the Europe-Afr.. |