| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
| Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.460 % | 0.460 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.12 % | 0.12 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 6.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Melt Index of Compound | 6.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 46.0 MPa | 6670 psi | Type I, 5 mm/min; ASTM D638 |
| 47.0 MPa | 6820 psi | 5 mm/min; ISO 527 | |
| Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 5 mm/min; ASTM D638 |
| 55.0 MPa | 7980 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 15.4 % | 15.4 % | 5 mm/min; ISO 527 |
| 19 % | 19 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 4.5 % | 4.5 % | Type I, 5 mm/min; ASTM D638 |
| 4.6 % | 4.6 % | 5 mm/min; ISO 527 | |
| Tensile Modulus | 3.20 GPa | 464 ksi | 1 mm/min; ISO 527 |
| 3.30 GPa | 479 ksi | 5 mm/min; ASTM D638 | |
| Flexural Yield Strength | 104 MPa | 15100 psi | 2 mm/min; ISO 178 |
| 105 MPa | 15200 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.83 GPa | 410 ksi | 2 mm/min; ISO 178 |
| 2.85 GPa | 413 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 2.60 J/cm | 4.87 ft-lb/in | ASTM D256 |
| 1.66 J/cm @Temperature -30.0 °C |
3.11 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*3; ISO 180/1A |
| 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB | NB | 80*10*3; ISO 180/1U |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
80*10*3; ISO 180/1U | |
| Charpy Impact Unnotched | NB | NB | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
| Charpy Impact, Notched | 2.50 J/cm² | 11.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 48.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 48.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 137 °C @Thickness 3.20 mm |
279 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 146 °C | 295 °F | Rate B/50; ASTM D1525 |
| 146 °C | 295 °F | Rate B/50; ISO 306 | |
| 148 °C | 298 °F | Rate B/120; ISO 306 |