Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.40 GPa | 638 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® RCM6123 PC+ABS (Asia Pacific) Cycoloy* RCM6123 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | ASTM D638 |
North Wood Plastics HDPE with 60% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 215 W1 902176 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, weather-stabilized |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 130, conditioning .. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | Conditioned; ISO 527-1,-2 |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.40 GPa @Temperature 80.0 °C |
638 ksi @Temperature 176 °F |
1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 30YK270 PP SABIC® STAMAX 30YK270 is a 30% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Asia Pacific) NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Europe-Africa-Middle East) NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE) LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1410V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1410V resin is a blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 10 % glass reinforcement. The resin is suitable for injection molding. Noryl GFN1410V resin has.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-2H PA12-GF20 Product description: Grilamid LV-2H is a 20% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 1mm/min; D638 |
Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced TECAPEEK® ST is a multipurpose semi-crystaline material from the polyaryletherketone family based on PEKEKK that features improved mechanical properties at higher temperatures. The benefits of TECA.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | Storage |
Epoxy Technology EPO-TEK® E2036 Epoxy Product Description: A two component, slightly flexible, silver-filled, electrically conductive adhesive for semiconductor and electronic assemblies. It is a low Tg epoxy, intended for many kinds o.. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 1 mm/min; ISO 527 |
Eurostar Star X RF003IU2-BK3047 PA66, Glass Fiber Filled, Impact Modified, Injection Molded Star X RF003IU2-BK3047 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66/6 Injection Molding (also known as Star X D 1010 14V/3/047)Information provided by Eurostar. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | |
BASF Procom® D 1012 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX2391 PPE+HIPS (Europe-Africa-Middle East) PX2391 is a 10% glass fiber reinforced, heat stabilized, low odor and low emission NORYL(R) grade for interior automotive applications, especially instrument panels |
|||
Tensile Modulus | 4.40 GPa | 638 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |