Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced

Category Polymer , Thermoplastic , Polyketone , Polyetherketoneetherketoneketone (PEKEKK), Wear Resistant
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECAPEEK® ST is a multipurpose semi-crystaline material from the polyaryletherketone family based on PEKEKK that features improved mechanical properties at higher temperatures. The benefits of TECAPEEK® ST compared to standard TECAPEEK® are that of a higher heat distortion temperature (HDT), better strength and stiffness of machined components and a higher flexural strength combined with a higher glass transition point.Excellent mechanical properties at higher temperaturesHigh heat distortion temperatureExcellent chemical resistanceLow moisture absorptionElectrically insulatingEasy to machine (unfilled)Good dimensional stabilityHigh purityTarget industries for TECAPEEK® ST are Oil and Gas, Semiconductor, Chemical and Automotive, crude petroleum extraction and drilling. Possible applications include turbocharger impellers, seal rings and other down hole parts, gears, and test sockets.Information Provided by Ensinger Inc.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
D792
Density 1.30 g/cc
0.0470 lb/in³
D792
Moisture Absorption at Equilibrium 0.050 %
0.050 %
RH 50%; D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 130 MPa
18900 psi
D638
Elongation at Yield 11 %
11 %
ISO527
Tensile Modulus 4.40 GPa
638 ksi
1mm/min; D638
Charpy Impact 5.80 J

@Temperature 22.8 °C
4.28 ft-lb

@Temperature 73.0 °F
ISO179
Thermal Properties Metric English Comments
CTE, linear 49.0 µm/m-°C
27.2 µin/in-°F
E831
Melting Point 387 °C
729 °F
D3418
Maximum Service Temperature, Air 260 °C
500 °F
Deflection Temperature at 1.8 MPa (264 psi) 172 °C
342 °F
D648
Glass Transition Temp, Tg 162 °C
324 °F
D3418
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC60093
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
IEC60093