Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.90 GPa | 566 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 500RS PC (Europe-Africa-Middle East) LEXAN 500RS is a medium viscosity, glass reinforced, flame retardant grade. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 503RS PC (Europe-Africa-Middle East) LEXAN 503RS is a medium viscosity, glass reinforced, flame retardant grade UV stabilized grade. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | ASTM D638 |
North Wood Plastics Polypropylene with 40% Wood Fiber, Extrusion Grade Data provided by North Wood Plastics, Inc. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL4019 PC Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL4019 PC (Asia Pacific) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Tensile Modulus | 3.90 GPa @Temperature 23.0 °C |
566 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 150P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact complian.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP 2802/30 000000 Nylon 66, 30% Glass Fiber PA 66 injection molding grade, 30% glass fibers, UL 94V-2 at 0.75 mm , GWFI:960°C at 0.75 mm, GWIT: 775°C at 0,75 mm, halogen-freeApplication Examples: mixer insert for blenders, washing machi.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | ASTM D638 |
Solvay Specialty Polymers PrimoSpire® PR-351 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-351 resin is a higher flow, injection molding grade of PrimoSpire® self-reinforced polyphenylene (SRP). PrimoSpire® SRP resin is an ultra-high performance amorphous, melt-pro.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | ISO 527 |
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | ISO 527 |
Polyram RamOfin PPH316G4 Polypropylene, 20% Glass Fiber 20% Glass fiber reinforced, high heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | |
Covestro Makroblend® UT-620 G Polycarbonate + Polyester Blend Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® AS V0 PA66 Product description: Grilon AS V0 is an unreinforced, normal viscosity, self-extinguishing PA66 injection molding grade. Grilon AS V0 has the following important properties: Halogen and phosphorous-.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 50mm/min; ISO 527-1 |
Denka TE-30 Transparent Resin Polymer (MABS resin) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Tensile Modulus | 3.90 GPa @Temperature 23.0 °C |
566 ksi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT 4011 Polyimide, Yellow (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Tensile Modulus | 3.90 GPa @Temperature 23.0 °C |
566 ksi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT™ 2061 Polyimide, 15% Graphite, 10% PTFE Filled (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Conditioned) Ultramid 1403-2 NF3001 is a 13% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, Conditioned Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | ISO 527 - 1 & - 2 |
Asahi Kasei Tenac® GA510 Homopolymer Acetal Resin 10% Glass fiber filled grade with high stiffness and superior dimensional stability.Information provided by Asahi Kasei Corporation. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 1mm/min; ISO 527 |
Teijin Panlite® GV-3410R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin GF 10% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis.. |
|||
Tensile Modulus | 3.90 GPa @Temperature -100 °C |
566 ksi @Temperature -148 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 1mm/min; ISO 527 |
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Conditioned) Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G .. |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPC343G20 Polypropylene Copolymer, 20% Glass Filled SAXALEN PPC343G20 is a 20% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |
|||
Tensile Modulus | 3.90 GPa | 566 ksi | ISO 527 |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |