Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger TECASINT 4011 Polyimide, Yellow (PI)

Category Polymer , Thermoplastic , Polyimide, Thermoplastic
Manufacturer Ensinger
Trade Name TECASINT
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ensinger TECASINT 4011 Polyimide, Yellow (PI).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.Main features: Very high thermal and oxidative resistance, high creep resistant, good radiation-resistance, high toughness, very good chemical resistance, very low absorption of water, low outgassing, good electrical insulating, easily machined, sensitive to hydrolysis in higher thermal range, flame retardant according to UL94 V-0Applications: Mechanical engineering, precision engineering, semiconductor, electronics, conveyor technology, electrical engineeringPreferred Fields: Valve seating, seals, insulators, lead backer, carriage, test socketsInformation Provided by Ensinger Sintimid
Physical Properties Metric English Comments
Density 1.416 g/cc
0.05116 lb/in³
DIN 53 479
Water Absorption 0.16 %
<br>@Temperature 23.0 °C
0.16 %
<br>@Temperature 73.4 °F
24 hours in water; EN ISO 62
0.60 %
<br>@Temperature 80.0 °C
0.60 %
<br>@Temperature 176 °F
24 hours in water; EN ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 88
<br>@Temperature 23.0 °C
88
<br>@Temperature 73.4 °F
DIN 53 505
Tensile Strength 124 MPa
<br>@Temperature 23.0 °C
18000 psi
<br>@Temperature 73.4 °F
EN ISO 527
Elongation at Break 4.5 %
<br>@Temperature 23.0 °C
4.5 %
<br>@Temperature 73.4 °F
EN ISO 527
Elongation at Yield 7.5 %
<br>@Temperature 23.0 °C
7.5 %
<br>@Temperature 73.4 °F
Flexural Elongation; EN ISO 178
Tensile Modulus 3.90 GPa
<br>@Temperature 23.0 °C
566 ksi
<br>@Temperature 73.4 °F
EN ISO 527
Flexural Strength 197 MPa
<br>@Temperature 23.0 °C
28600 psi
<br>@Temperature 73.4 °F
EN ISO 178
Flexural Modulus 4.316 GPa
<br>@Temperature 23.0 °C
626.0 ksi
<br>@Temperature 73.4 °F
EN ISO 178
Compressive Yield Strength 185 MPa
<br>@Strain 10.0 %,<br> Temperature 23.0 °C
26800 psi
<br>@Strain 10.0 %,<br> Temperature 73.4 °F
EN ISO 604
Compressive Strength 570 MPa
<br>@Temperature 23.0 °C
82700 psi
<br>@Temperature 73.4 °F
EN ISO 604
Compressive Modulus 2.36 GPa
<br>@Temperature 23.0 °C
342 ksi
<br>@Temperature 73.4 °F
EN ISO 604
Charpy Impact Unnotched 7.20 J/cm²
<br>@Temperature 23.0 °C
34.3 ft-lb/in²
<br>@Temperature 73.4 °F
EN ISO 179
Compression Set 70 %
<br>@Temperature 23.0 °C
70 %
<br>@Temperature 73.4 °F
Compression at Break; EN ISO 604
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C
<br>@Temperature 50.0 - 200 °C
25.0 µin/in-°F
<br>@Temperature 122 - 392 °F
DIN 53 752
CTE, linear, Transverse to Flow 57.0 µm/m-°C
<br>@Temperature 50.0 - 200 °C
31.7 µin/in-°F
<br>@Temperature 122 - 392 °F
DIN 53 752
Specific Heat Capacity 1.04 J/g-°C
0.249 BTU/lb-°F
Thermal Conductivity 0.400 W/m-K
<br>@Temperature 40.0 °C
2.78 BTU-in/hr-ft²-°F
<br>@Temperature 104 °F
ISO 8302
Glass Transition Temp, Tg 260 °C
500 °F
DSC
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
<br>@Temperature 23.0 °C
1.00e+16 ohm-cm
<br>@Temperature 73.4 °F
IEC 60093
Surface Resistivity per Square 1.00e+16 ohm
<br>@Temperature 23.0 °C
1.00e+16 ohm
<br>@Temperature 73.4 °F
IEC 60093
Dielectric Strength 18.0 kV/mm
<br>@Temperature 23.0 °C
457 kV/in
<br>@Temperature 73.4 °F
ISO 60243-1
Copyright © lookpolymers.com All Rights Reserved