Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.59 GPa | 521 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Trilliant™ HC HC6600-0010 ESD Black Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | >= 3.59 GPa | >= 521 ksi | ISO 527-1,2 |
Qualchem Danamid AFES-21 Polyamide 66 Impact resistant, dryInformation provided by Qualchem Zrt. |
|||
Tensile Modulus | 3.59 GPa | 520 ksi | ASTM D638 |
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OL003A PPS - Branched LNP* LUBRICOMP* OL003A is a compound based on PPS - Branched resin containing 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010A PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010A PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010K PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010K PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010KM PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010RF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 9011 PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). Resin is RoHS compliant. Improved processability for Fiber extrusion. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU1000E PEI Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | ASTM Test |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Conditioned) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX8410W PPE+PA High flow, 10% Glass Reinforced PPE+PA. Typically used in Automotive connectors. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010KM PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM AUT200 PEI Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperat.. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM AUT210 PEI Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti.. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Tensile Modulus | 3.59 GPa | 520 ksi | ASTM D638 |
Westlake Plastics PEEK PEEK is a high performance semi-crystalline thermoplastic. PEEK characteristics include high temperature performance, excellent wear properties, superior chemical resistance and outstanding toughne.. |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | |
Hexcel® F161 Epoxy Resin F161 is a structural, heat resistant and electrical grade epoxy formulation designed for autoclave curing. F161 is a high temperature, laminate grade epoxy resin with a 350ºF (177ºC) cure. F161 is.. |
|||
Tensile Modulus | 3.59 GPa @Temperature 150 °C |
520 ksi @Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Modulus | 3.59 GPa | 520 ksi | ASTM D638 |
Asahi Kasei Thermylene® P6-40FB-Y947 40% Glass Fiber/Glass Bead, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Modulus | 3.59 GPa | 521 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1000EF PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS. US FDA and EU Food Contact compliant. |
|||
Tensile Modulus | 3.59 GPa | 520 ksi | ASTM D638 |
ScanTube PEEK Tubing Information provided by ScanTube, Inc. |