Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ScanTube PEEK Tubing

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer ScanTube
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ScanTube PEEK Tubing.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by ScanTube, Inc.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ASTM D792
Water Absorption <= 0.50 %
<= 0.50 %
ASTM D257
Mechanical Properties Metric English Comments
Hardness, Rockwell R 126
126
Elongation at Break 50 %
50 %
ASTM D638, ASTM D1708
Tensile Modulus 3.59 GPa
520 ksi
ASTM D638
Flexural Modulus 3.65 GPa
530 ksi
ASTM D790
Compressive Strength 118 MPa
17100 psi
ASTM D695
Thermal Properties Metric English Comments
Thermal Conductivity 0.173 W/m-K
1.20 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 334 °C
633 °F
Maximum Service Temperature, Air 250 °C
482 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
286 °F
ASTM D648
Flammability, UL94 V-0
V-0
Oxygen Index 35 %
35 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Dielectric Strength >= 19.7 kV/mm
>= 500 kV/in
Short Term; 10 mil film; ASTM D149
Descriptive Properties Value Comments
Chemical Resistance Excellent
Weather Resistance Excellent
Users viewing this material also viewed the following: