Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.96 GPa @Thickness 3.20 mm |
284 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Modulus | 1.96 GPa @Thickness 3.20 mm |
284 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Tensile Modulus | 1.96 GPa @Thickness 3.20 mm |
284 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp IP003 PA6.12 LNP* Lubricomp* IP003 is a Nylon 6/12 base resin containing PTFE and Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7727 PP SABIC® PPcompound 7727 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, heat stability, and is used in injection molded applications. The IMDS ID.. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 3706 PBT+PC Impact modified PBT+PC resin. Outdoor enclosure. Not available in all colors. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66 LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA11 LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing 30% Glass Bead. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® CF-1030 PC, Unreinforced High Impact Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® EA-0640 ABS, Unreinforced Permanent static prevention ABS material such as LCD carrierInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® CF-1051 PC, Unreinforced High Impact High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HP-1000H PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HP-1000P PC/ABS, Unreinforced High flow material that can be used in the exterior material of mobile phone, wheel cap, rice cooker, electric iron etc. as well as refrigerator door handle and panelInformation provided by Samsung .. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® EA-0640 ABS, Unreinforced Permanent static prevention ABS material such as LCD carrierInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SD-0150UF ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HP-1000P PC/ABS, Unreinforced High flow material that can be used in the exterior material of mobile phone, wheel cap, rice cooker, electric iron etc. as well as refrigerator door handle and panelInformation provided by Samsung .. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | ASTM D882 |
Westlake Plastics ECTFE Film Made from HALAR® Ethylene-chlorotrifluoroethylene Resin Excellent purity. Excellent chemical resistance. Low permeability. Excellent abrasion resistance. Excellent temperature resistance.Halar® is a trade name of Solvay Solexis, Inc. Information p.. |
|||
Tensile Modulus | 1.96 GPa @Temperature -100 °C |
284 ksi @Temperature -148 °F |
50%RH; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.96 GPa | 284 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® CF-1030 PC, Unreinforced High Impact Information provided by Samsung Cheil Industries. |