Category | Polymer , Thermoplastic , Nylon |
Manufacturer | DuPont Performance Polymers |
Trade Name | Zytel® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | DuPont Performance Polymers Zytel® 330 NC010 Nylon (Unverified Data**).pdf |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 g/cc | 0.0426 lb/in³ | DAM; ISO 1183 |
Water Absorption | 5.8 % @Thickness 2.00 mm |
5.8 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
Viscosity | 44000 cP @Shear Rate 5000 1/s, Temperature 320 °C |
44000 cP @Shear Rate 5000 1/s, Temperature 608 °F |
ISO 11403-1 -2 |
70000 cP @Shear Rate 500 1/s, Temperature 320 °C |
70000 cP @Shear Rate 500 1/s, Temperature 608 °F |
ISO 11403-1 -2 | |
72000 cP @Shear Rate 5000 1/s, Temperature 300 °C |
72000 cP @Shear Rate 5000 1/s, Temperature 572 °F |
ISO 11403-1 -2 | |
122000 cP @Shear Rate 5000 1/s, Temperature 280 °C |
122000 cP @Shear Rate 5000 1/s, Temperature 536 °F |
ISO 11403-1 -2 | |
127000 cP @Shear Rate 500 1/s, Temperature 300 °C |
127000 cP @Shear Rate 500 1/s, Temperature 572 °F |
ISO 11403-1 -2 | |
243000 cP @Shear Rate 500 1/s, Temperature 280 °C |
243000 cP @Shear Rate 500 1/s, Temperature 536 °F |
ISO 11403-1 -2 | |
Viscosity Test | 80 cm³/g | 80 cm³/g | DAM; ISO 307 1157 1628 |
Linear Mold Shrinkage, Flow | 0.0050 cm/cm | 0.0050 in/in | DAM; ISO 294-4 2577 |
Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | DAM; ISO 294-4 2577 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 97.0 MPa | 14100 psi | DAM; ISO 527-1/-2 |
Elongation at Break | >= 50 % | >= 50 % | DAM; Nominal; ISO 527-1/-2 |
Elongation at Yield | 6.0 % | 6.0 % | DAM; ISO 527-1/-2 |
Tensile Modulus | 1.30 GPa | 189 ksi | 50%RH; ISO 527-1/-2 |
2.40 GPa | 348 ksi | DAM; ISO 527-1/-2 | |
0.000701 GPa @Temperature 170 °C |
0.102 ksi @Temperature 338 °F |
50%RH; Dynamic; ISO 11403-1 -2 | |
0.00208 GPa @Temperature 170 °C |
0.302 ksi @Temperature 338 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
0.0387 GPa @Temperature 110 °C |
5.61 ksi @Temperature 230 °F |
50%RH; Dynamic; ISO 11403-1 -2 | |
1.27 GPa @Temperature 30.0 °C |
184 ksi @Temperature 86.0 °F |
50%RH; Dynamic; ISO 11403-1 -2 | |
1.40 GPa @Temperature -20.0 °C |
202 ksi @Temperature -4.00 °F |
50%RH; Dynamic; ISO 11403-1 -2 | |
1.4027 GPa @Temperature 110 °C |
203.44 ksi @Temperature 230 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
1.58 GPa @Temperature 30.0 °C |
230 ksi @Temperature 86.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
1.70 GPa @Temperature -70.0 °C |
246 ksi @Temperature -94.0 °F |
50%RH; Dynamic; ISO 11403-1 -2 | |
1.72 GPa @Temperature -20.0 °C |
250 ksi @Temperature -4.00 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
1.96 GPa @Temperature -100 °C |
284 ksi @Temperature -148 °F |
50%RH; Dynamic; ISO 11403-1 -2 | |
2.06 GPa @Temperature -70.0 °C |
299 ksi @Temperature -94.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
2.24 GPa @Temperature -100 °C |
325 ksi @Temperature -148 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | DAM; ISO 180/1A |
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | DAM; ISO 179/1eU |
NB | NB | 50%RH; ISO 179/1eU | |
18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
23.0 J/cm² @Temperature -40.0 °C |
109 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eU | |
Charpy Impact, Notched | 0.990 J/cm² | 4.71 ft-lb/in² | DAM; ISO 179/1eA |
1.20 J/cm² | 5.71 ft-lb/in² | 50%RH; ISO 179/1eA | |
0.450 J/cm² @Temperature -30.0 °C |
2.14 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
0.450 J/cm² @Temperature -40.0 °C |
2.14 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA | |
Puncture Energy | 37.0 J @Load 377 kg |
27.3 ft-lb @Load 832 lb |
50%RH; ISO 6603-2 |
70.0 J @Load 561 kg |
51.6 ft-lb @Load 1240 lb |
DAM; ISO 6603-2 | |
19.0 J @Load 316 kg, Temperature -30.0 °C |
14.0 ft-lb @Load 697 lb, Temperature -22.0 °F |
50%RH; ISO 6603-2 | |
47.0 J @Load 438 kg, Temperature -30.0 °C |
34.7 ft-lb @Load 967 lb, Temperature -22.0 °F |
DAM; ISO 6603-2 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 62.0 µm/m-°C | 34.4 µin/in-°F | DAM; ISO 11359-1/-2 |
CTE, linear, Transverse to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | DAM; ISO 11359-1/-2 |
Specific Heat Capacity | 2.46 J/g-°C | 0.588 BTU/lb-°F | |
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | of melt |
Deflection Temperature at 0.46 MPa (66 psi) | 127 °C | 261 °F | DAM; ISO 75-1/-2 |
Deflection Temperature at 1.8 MPa (264 psi) | 123 °C | 253 °F | DAM; ISO 75-1/-2 |
Glass Transition Temp, Tg | 140 °C | 284 °F | DAM; 10°C/min; ISO 11357-1/-2 |
Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; IEC 60695-11-10 |
V-2 @Thickness 0.900 mm |
V-2 @Thickness 0.0354 in |
DAM; IEC 60695-11-10 |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Transmission, Visible | 88 % | 88 % | ISO 13468-1 -2 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | DAM; IEC 60093 |
1.00e+15 ohm-cm | 1.00e+15 ohm-cm | 50%RH; IEC 60093 | |
Dielectric Constant | 3.7 @Frequency 1.00e+6 Hz |
3.7 @Frequency 1.00e+6 Hz |
DAM; IEC 60250 |
3.8 @Frequency 1.00e+6 Hz |
3.8 @Frequency 1.00e+6 Hz |
50%RH; IEC 60250 | |
4.1 @Frequency 100 Hz |
4.1 @Frequency 100 Hz |
DAM; IEC 60250 | |
4.3 @Frequency 100 Hz |
4.3 @Frequency 100 Hz |
50%RH; IEC 60250 | |
Dielectric Strength | 28.0 kV/mm | 711 kV/in | 50%RH; IEC 60243-1 |
29.0 kV/mm | 737 kV/in | DAM; IEC 60243-1 | |
Dissipation Factor | 0.020 @Frequency 100 Hz |
0.020 @Frequency 100 Hz |
DAM; IEC 60250 |
0.020 @Frequency 100 Hz |
0.020 @Frequency 100 Hz |
50%RH; IEC 60250 | |
0.020 @Frequency 1.00e+6 Hz |
0.020 @Frequency 1.00e+6 Hz |
DAM; IEC 60250 | |
0.020 @Frequency 1.00e+6 Hz |
0.020 @Frequency 1.00e+6 Hz |
50%RH; IEC 60250 | |
Comparative Tracking Index | 600 V | 600 V | DAM; IEC 60112 |
Descriptive Properties | Value | Comments |
---|---|---|
Delivery Form | Pellets | |
Part Marking Code | >PA< | ISO 11469 |
Processing | Injection Moulding | |
Regional Availability | Europe | |
Near East/Africa | ||
North America | ||
South and Central America | ||
Resin Identification | PA | |
Special Characteristics | Heat stabilised or stable to heat | |
Transparent |