Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BP Amoco Accpro® 9346 Enhanced Polypropylene  (discontinued **)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BP Amoco Accpro® 9346 Enhanced Polypropylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Suggested fabrication methods: Injection moldingFeatures: Long-term heat aging, High stiffness, Nucleated, UL RecognizedComplies with FDA specification, Title 21, CFR 177.1520.Typical applications: AppliancesTypical property data below from injection molded samples.
Physical Properties Metric English Comments
Density 0.886 - 0.926 g/cc
0.0320 - 0.0335 lb/in³
ASTM D1505
Water Absorption <= 0.010 %
<= 0.010 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 43.0 MPa
6240 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790A
Izod Impact, Notched 0.320 J/cm

@Diameter 3.17 mm
0.599 ft-lb/in

@Diameter 0.125 in
bar
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
UL Relative Thermal Index
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648
Flammability, UL94 HB
HB