Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
ASTM D638 |
LG Chemical LUMILOY GN1006F Injection Molding FR mPPO Uses include electric/electronic parts. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-0300 ABS, Unreinforced FR Flame-retardant non-halogen ABS with superior heat resistance that can be used in the interior/exterior material of CD/DVD-Combo and DVD-RecordersInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-0825 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SR-7300 ABS/PET, Unreinforced Material with superior chemical resistance that can be used in the interior/exterior material of household appliances that require heat resistanceInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TX-0530T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® CR-0760 ABS, Unreinforced Good chemical resistanceInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SR-7300 ABS/PET, Unreinforced Material with superior chemical resistance that can be used in the interior/exterior material of household appliances that require heat resistanceInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0860EX ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0860EX ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | ASTM D638 |
SCG Chemicals EL-Proâ„¢ P702J Polypropylene Injection Molding Key Characteristics:High clarityHigh stiffnessGood processabilityMicrowavable for cooking applicationsOdorlessSafe for food contactRecommended Applications:General purpose injection parts that requi.. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | ASTM D638M |
Total PSC 1540(AS) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron HCR-15 M ABS Heat Resistant Chemical Resistant GradeInformation provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron IM-18 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron AN-450 EVM Flame Retardant ABS Grade Information provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron AN-450 Flame Retardant ABS Grade Information provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron IM-18 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron AN-450 EVM Flame Retardant ABS Grade Information provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade Electroplating, High FlowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade Electroplating, High FlowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron HCR-15 M ABS Heat Resistant Chemical Resistant GradeInformation provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1; ASTM D638 |
Bhansali Engineering Abstron MIF-45 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |