Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® NH-0300 ABS, Unreinforced FR

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® NH-0300 ABS, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flame-retardant non-halogen ABS with superior heat resistance that can be used in the interior/exterior material of CD/DVD-Combo and DVD-RecordersInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength, Yield 41.2 MPa
5970 psi
50 mm/min; ASTM D638
Flexural Strength 65.7 MPa
9530 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.35 GPa
341 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.86 J/cm

@Thickness 3.17 mm
3.49 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C

@Thickness 6.40 mm
207 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-2

@Thickness 0.750 - 3.00 mm
V-2

@Thickness 0.0295 - 0.118 in