Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled PC/ABS Alloy, General Purpose, 20% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PC/TP-GP2-G20 PC/Polyester Alloy, 20% Glass Reinforced Excellent Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PPX-G10 Modified-PPO, 10% Glass Reinforced Modified-Polyphenylene Oxide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources TP-GFMF2 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced Polybutylene Terephthalate, 40% Glass/Mineral ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PC/TP-GP2-G20 PC Polyester, Excellent Chemical Resistance, 20% Glass Filled
(Unverified Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Fiberfil® J-60/20/FR Polypropylene Homopolymer, 20% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Fiberfil® J-60/40 Polypropylene Homopolymer, 40% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Global GPP-130-C 30% Glass Filled Chemically Coupled Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 72.4 MPa @Temperature 25.0 °C |
10500 psi @Temperature 77.0 °F |
|
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |
|||
Tensile Strength, Yield | >= 72.4 MPa | >= 10500 psi | |
H.C. Starck Grain Stabilized Niobium (GSNb) GSNb is a patent pending single-phase micro-alloy that has a grain size of approximately 2 ASTM numbers finer than standard commercial grade niobium.Applications: Grain Stabilized Niobium (GSNb) is.. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES HiFill FR® ABS GF30 FR 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GB30 FR 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: LubricantFeatures: Flame Retardant and LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES HiFill® ABS GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES HiFill® ABS GF10 LE 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES HiFill® PA11 GB7 HS L 7% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 7% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by T.. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES HiFill® PA6 0137 S2 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 0137 S2 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES HiFill® PP GF/M50 CC BK 50% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES Luriblend® PA6 GL10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant(10%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES Luriblend® POM CO GF10 TL10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionApp.. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | Resin property; RT; Dry |
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l.. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | |
Tra-Con Tra-Bond 2248 High Temperature Epoxy Staking Adhesive TRA-BOND 2248 is a thixotropic, high temperature cure, 100% solids epoxy resin system that provides strong, tough bonds between a wide range of materials (includes metals, glass, ceramics, and many .. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Asahi Kasei Thermylene® F6-30FG-0100 30% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Asahi Kasei Thermylene® P-30FG-0812 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | |
Asahi Kasei Thermylene® P7-20FG-0876 Chemically Coupled Polypropylene Compound, 20% Glass Filled Applications: Automotive: Sun Roof Rails, Fan Shrouds, Air Cleaners, Battery Boxes, Air Induction Components, Battery Trays, Blower Wheels, Light Housings, Shifter Bases, Interior Consoles, Arm Rest.. |
|||
Tensile Strength, Yield | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | >= 72.4 MPa | >= 10500 psi | ASTM D638 |
Spartech Polycast Poly FR9 (0.060") Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |