Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Global GPP-130-C 30% Glass Filled Chemically Coupled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global GPP-130-C 30% Glass Filled Chemically Coupled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 72.4 MPa
10500 psi
ASTM D638
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ASTM D648
Users viewing this material also viewed the following: